PPA AMODEL®  AF-4133 VO BK324 SOLVAY USA

327
  • Unit Price:US$ 5,988 /MT
  • Packaging Specification:
    25 KG/PKG
  • Packaging Material:
    Paper bag
  • Supply Quantity:
    43MT
  • Delivery Terms:
    FOB
  • Port of Loading :
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 ********View
serv********View
+86 ********View

For more details, please contact the supplier!

Material Description

  • Material Properties:Flame retardantHigh temperature resistanceFiller: Glass fiber reinforced material33% filler by weight
  • Application Areas:Automotive componentsElectronic and electrical componentsElectrical componentsElectrical/Electronic ApplicationsLaptop caseVehicle electronics
  • Color:--
  • Grade:Injection grade

Material Certification

UL

Technical Data Sheet

impact performanceTest ConditionTest MethodTest Result
Suspended wall beam without notch impact strength23°CISO 180/1U68 kJ/m²
Impact strength of simply supported beam without notch23°CISO 179/1eU79 kJ/m²
flammabilityTest ConditionTest MethodTest Result
UL flame retardant rating3.2mmUL 94HB
mechanical propertiesTest ConditionTest MethodTest Result
Bending strainISO 1783.1 %
bending strength23°CISO 178295 Mpa
Bending modulus23°CISO 17810700 Mpa
Tensile strainBreak,23°CISO 527-22.5 %
tensile strengthBreak,23°CISO 527-2210 Mpa
Tensile modulus23°CISO 527-212000 Mpa
thermal performanceTest ConditionTest MethodTest Result
Hot deformation temperature1.8MPa,UnannealedISO 75-2/A>300 °C
Glass transition temperatureDSC95.0 °C
Linear coefficient of thermal expansionTD:100to200°CASTME8311.2E-04 cm/cm/°C
Linear coefficient of thermal expansionTD:0to100°CASTME8317.6E-05 cm/cm/°C
Linear coefficient of thermal expansionMD:100to200°CASTME8311.5E-05 cm/cm/°C
Linear coefficient of thermal expansionMD:0to100°CASTME8312E-05 cm/cm/°C
Melting temperatureISO 11357-3327 °C
Physical propertiesTest ConditionTest MethodTest Result
Water absorption rate24hrASTM D5700.23 %
Shrinkage rateTDASTM D9550.80 %
Shrinkage rateMDASTM D9550.40 %
Electrical performanceTest ConditionTest MethodTest Result
Dissipation factor60HzASTM D1506E-03
Dielectric constant1MHzASTM D1503.75
Dielectric constant60HzASTM D1504.10
Dielectric strength3.20mmASTM D14919 KV/mm
Volume resistivityASTM D2575.6E+15 ohms·cm
High voltage arc tracing rateHVTRUL 746 mm/min
Compared to the anti leakage trace indexCTIUL 746PLC 0
Dissipation factor1MHzASTM D1500.015
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.