PC/ABS INFINO®  LS-1159 K21441 Samsung Cheil South Korea

198
  • Unit Price:US$ 4,035 /MT
  • Packaging Specification:
    25 KG/PKG
  • Packaging Material:
    Paper bag
  • Supply Quantity:
    24.8MT
  • Delivery Terms:
    FOB
  • Port of Loading :
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 ********View
serv********View

For more details, please contact the supplier!

Material Description

  • Material Properties:Glass fiber reinforcedFlame retardantFiller: Glass fiber reinforced material
  • Application Areas:Tool handleTV
  • Color:--
  • Grade:Injection grade

Technical Data Sheet Compare

physical property Test ConditionTest MethodTest Result
melt mass-flow rateASTM D123814 g/10min
melt mass-flow rateISO 113314 g/10min
Shrinkage rateASTM D9550.10 %
Shrinkage rateASTM D9550.10 %
Shrinkage rateISO 25770.10 %
Shrinkage rateISO 25770.10 %
ash contentISO 345115 %
ash contentASTM D563015 %
hardnessTest ConditionTest MethodTest Result
Rockwell hardnessASTM D785120
Rockwell hardnessISO 2039-2120
flammabilityTest ConditionTest MethodTest Result
UL flame retardant ratingUL 94V-1
UL flame retardant ratingUL 94V-0
UL flame retardant ratingUL 94V-0
UL flame retardant ratingUL 94V-0
Mechanical propertiesTest ConditionTest MethodTest Result
bending strengthASTM D790120 Mpa
bending strengthISO 178110 Mpa
Tensile modulusASTM D6384300 Mpa
Tensile modulusISO 527-2/54400 Mpa
tensile strength ASTM D63878.0 Mpa
tensile strength ISO 527-2/580.0 Mpa
tensile strength ASTM D63888.0 Mpa
tensile strength ISO 527-2/590.0 Mpa
elongationASTM D6383.3 %
Tensile strainISO 527-2/53.3 %
Flexural modulusASTM D7904700 Mpa
Flexural modulusISO 1785000 Mpa
Impact resistanceTest ConditionTest MethodTest Result
Charpy Notched Impact StrengthISO 179/1eA6.0 kJ/m²
Impact strength of cantilever beam gapISO 180/1A6.0 kJ/m²
Thermal performanceTest ConditionTest MethodTest Result
Heat distortion temperatureISO 75-2/A91.0 °C
vicatISO 306/B5097.0 °C
Heat distortion temperatureASTM D64896.0 °C
Heat distortion temperatureASTM D64891.0 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.