PA46 Stanyl® TS256F8 DSM HOLAND
188
- Unit Price:US$ 5,996 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:59MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
For more details, please contact the supplier!
Material Description
- Material Properties:Thermal stability|Flame retardant
- Application Areas:Casters|Automotive Applications
- Color:--
- Grade:Injection grade
Material Certification

Technical Data Sheet
other | Test Condition | Test Method | Test Result |
---|---|---|---|
characteristic | 吸潮性差 阻燃 玻纤增强 |
thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Combustibility (rate) | UL 94 | V-0 | |
melting temperature | ISO 3146 | 295 °C | |
Heat Deflection Temperature | 1.8MPa | ISO 75-1 | 290 °C |
Linear coefficient of thermal expansion | ISO 11359-2 | 0.00002 cm/cm/°C |
Basic performance | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ISO 1183 | 1.65 g/cm³ | |
Water absorption rate | 23°C/50%RH | ISO 62 | 1.3 % |
Other performance | Test Condition | Test Method | Test Result |
---|---|---|---|
UL flame retardant rating | UL 94 | V-0 |
Physical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ASTM D792/ISO 1183 | 1.65 | |
Water absorption rate | ASTM D570/ISO 62 | 1.3 % |
mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile modulus | ASTM D638/ISO 527 | 14000 kg/cm²(MPa)[Lb/in²] | |
Charpy Notched Impact Strength | 23°C | ISO 180-1A | 8.0 kJ/m² |
Impact strength of cantilever beam gap | 23°C | ISO 180-1A | 8.0 kJ/m² |
tensile strength | ISO 527-2 | 1800 Mpa |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.