PP Clyrell RC124H LYONDELLBASELL GERMANY
406
- Unit Price:US$ 2,307 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:26.5MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:High gloss|optical performance |high definition
- Application Areas:Monitor|Food packaging|Bag|film|chip
- Color:--
- Grade:--
Technical Data Sheet
| optical performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| gloss | 45°,50.0μm | ASTM D2457 | 91 |
| 45°,40.0μm,Blown Film | ASTM D2457 | 93 | |
| turbidity | 50.0μm | ASTM D1003 | <1.0 % |
| 40.0μm,Blown Film | ASTM D1003 | 1.0 % |
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Tensile modulus | ISO 527-2/1 | 750 Mpa | |
| tensile strength | Yield | ISO 527-2/50 | 25.0 Mpa |
| Tensile strain | Yield | ISO 527-2/50 | 15 % |
| Break | ISO 527-2/50 | 510 % |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 69.0 °C |
| Vicat softening temperature | ISO 306/A50 | 122 °C |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| melt mass-flow rate | 230°C/2.16kg | ISO 1133 | 2.2 g/10min |
| film | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Secant modulus | MD | ASTM D882 | 600 Mpa |
| MD:40μm,Blown Film2 | ASTM D882 | 840 Mpa | |
| TD:40μm,Blown Film2 | ASTM D882 | 860 Mpa | |
| tensile strength | MD:Yield | ASTM D882 | 18.0 Mpa |
| MD:Yield,40μm,Blown Film3 | ASTM D882 | 27.0 Mpa | |
| TD:Yield,40μm,Blown Film3 | ASTM D882 | 25.0 Mpa | |
| MD:Break | ASTM D882 | 40.0 Mpa | |
| MD:Break,40μm,Blown Film3 | ASTM D882 | 31.0 Mpa | |
| TD:Break,40μm,Blown Film3 | ASTM D882 | 27.0 Mpa | |
| elongation | MD:Yield,40μm,Blown Film3 | ASTM D882 | 9.0 % |
| TD:Yield,40μm,Blown Film3 | ASTM D882 | 8.0 % | |
| MD:Break | ASTM D882 | 730 % | |
| MD:Break,40μm,Blown Film3 | ASTM D882 | 590 % | |
| TD:Break,40μm,Blown Film3 | ASTM D882 | 540 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.