PP-R YUHWA POLYPRO® RP2400 KOREA PETROCHEMICAL
365
- Unit Price:US$ 1,254 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:20MT
- Delivery Terms:FOB
- Port of Loading :Shenzhen Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:Processability
- Application Areas:Pipe fittings|Pipeline system
- Color:--
- Grade:Injection grade
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of cantilever beam gap | ASTM D256 | 无断裂 | ||
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| tensile strength | Yield | ASTM D638 | 22.6 | Mpa |
| elongation | Break | ASTM D638 | >600 | % |
| Bending modulus | ASTM D790 | 834 | Mpa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Hot deformation temperature | 1.8MPa,Unannealed | ASTM D648 | 85.0 | °C |
| Vicat softening temperature | ASTM D1525 | 133 | °C | |
| Melting temperature | ASTM D3418 | 139 | °C | |
| Oxygen induction time | 200°C | ASTM D3895 | >30 | min |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| density | ASTM D1505 | 0.900 | g/cm³ | |
| melt mass-flow rate | 230°C/2.16kg | ASTM D1238 | 0.25 | g/10min |
| ash content | ASTM D5630 | <300 | ppm | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Rockwell hardness | R-Scale | ASTM D785 | 72 | |
| Supplementary Information | Test Condition | Test Method | Test Result | Test Unit |
| Minimum Required Strength (MRS) | ISO 9080 | 11.2 | Mpa |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.