plas

PETG Eastar™  DS2010 EASTMAN USA

892
  • Unit Price:US$ 2,045 /MT
  • Packaging Specification:
    25 KG/PKG
  • Packaging Material:
    Paper bag
  • Supply Quantity:
    100.5MT
  • Delivery Terms:
    FOB
  • Port of Loading :
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 ********View
serv********View
+86 ********View

For more details, please contact the supplier!

Material Description

  • Material Properties:High transparencyHigh toughness
  • Application Areas:sporting goodschip
  • Color:--
  • Grade:Injection grade

Material Certification

UL

Technical Data Sheet

optical performanceTest ConditionTest MethodTest Result
turbidityASTM D10030.30 %
transmissivityRegularASTM D100389.0 %
transmissivityTotalASTM D100391.0 %
impact performanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gap23°CISO 18030 kJ/m²
Impact strength of cantilever beam gap-40°CASTM D4812NoBreak
Impact strength of cantilever beam gap23°CASTM D4812NoBreak
Impact strength of cantilever beam gap-40°CISO 1806.3 kJ/m²
Impact strength of cantilever beam gap23°CASTM D256370 J/m
Impact strength of cantilever beam gap-40°CASTM D25660 J/m
Dart impact-40°C,EnergyatPeakLoadASTM D376348.0 J
Dart impact23°C,EnergyatPeakLoadASTM D376345.0 J
Multi axis Instrumented Impact Energy-40°C,能量to力量峰值ISO 6603-255.0 J
Multi axis Instrumented Impact Energy23°C,能量to力量峰值ISO 6603-271.0 J
flammabilityTest ConditionTest MethodTest Result
UL flame retardant rating3.0mmUL 94V-2
mechanical propertiesTest ConditionTest MethodTest Result
bending strengthYield,23°CASTM D79067.0 Mpa
bending strength23°CISO 17864.0 Mpa
Bending modulus23°CISO 1781750 Mpa
Bending modulus23°CASTM D7901900 Mpa
tensile strengthYield,23°CASTM D63846.0 Mpa
tensile strengthYield,23°CISO 527-247.0 Mpa
tensile strengthBreak,23°CASTM D63853.0 Mpa
tensile strengthBreak,23°CISO 527-249.0 Mpa
elongationYield,23°CASTM D6385.0 %
Tensile strainYield,23°CISO 527-24.0 %
elongationBreak,23°CASTM D638310 %
Tensile strainBreak,23°CISO 527-2210 %
thermal performanceTest ConditionTest MethodTest Result
Hot deformation temperature0.45MPa,UnannealedASTM D64873.0 °C
Hot deformation temperature0.45MPa,UnannealedISO 75-2/B73.0 °C
Hot deformation temperature1.8MPa,UnannealedASTM D64865.0 °C
Hot deformation temperature1.8MPa,UnannealedISO 75-2/A66.0 °C
Physical propertiesTest ConditionTest MethodTest Result
densityASTM D7921.20 g/cm³
density23°CISO 11831.19 g/cm³
Shrinkage rateMD:3.20mmASTM D9550.20-0.60 %
Electrical performanceTest ConditionTest MethodTest Result
Dissipation factor23°C,1MHzASTM D1500.015
Dissipation factor23°C,100kHzASTM D1500.015
Dissipation factor23°C,10kHzASTM D1500.012
Dissipation factor23°C,1kHzASTM D1506E-03
Dielectric constant23°C,1MHzASTM D1502.50
Dielectric constant23°C,100kHzASTM D1502.50
Dielectric constant23°C,10kHzASTM D1502.60
Dielectric constant23°C,1kHzASTM D1502.60
Dielectric strength23°CASTM D14917 KV/mm
Volume resistivity23°CASTM D2571E+17 ohms·cm
Compared to the anti leakage trace indexASTM D3638PLC 0
Arc resistanceASTM D495123 sec
Surface resistivityASTM D2571E+17 ohms
hardnessTest ConditionTest MethodTest Result
Rockwell hardnessR-Sale,23°CASTM D785105
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.