PMMA ACRYPET™ MF001 MITSUBISHI NANTONG
430
- Unit Price:US$ 2,092 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:268.7MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
- Material Comparison:PMMA ACRYREX® CM-211 TAIWAN CHIMEI
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
For more details, please contact the supplier!
Material Description
- Material Properties:heat-resisting|High temperature resistance|High mobility|transparent| High heat resistance
- Application Areas:Household appliances|Household appliances|Casters|Optical level
- Color:--
- Grade:Withdrawal level
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
transmittance | ASTM D-1003 | MF|93 % | |
ASTM D-1003 | 93 % | ||
density | ATSM D-792 | MF|1.19 | |
ATSM D-792 | 1.19 | ||
refractive index | ASTM D-542 | MF|1.49 | |
ASTM D-542 | 1.49 |
Basic performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Water absorption rate | ASTM D-570 | MF|0.3 % | |
ASTM D-570 | 0.3 % | ||
melt mass-flow rate | ASTM D-1238 | MF|14 g/10min | |
ASTM D-1238 | 2.5 g/10min |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Rockwell hardness | ASTM D-785 | MF|90 M Scale | |
ASTM D-785 | 95 M Scale | ||
elongation at break | ASTM D-638 | MF|4 % | |
ASTM D-638 | 5 % | ||
Impact strength of cantilever beam gap | ASTM D-255 | MF|1.6 kg·cm/cm | |
ASTM D-255 | 1.6 kg·cm/cm | ||
tensile strength | ASTM D-638 | MF|670 kg/cm2 | |
ASTM D-638 | 730 kg/cm2 | ||
compressive strength | ASTM D-695 | MF|1000 kg/cm2 | |
ASTM D-695 | 1100 kg/cm2 | ||
Flexural modulus | ASTM D-790 | MF|3.1×104 kg/cm2 | |
ASTM D-790 | 3.1×104 kg/cm2 | ||
bending strength | ASTM D-790 | MF|1000 kg/cm2 | |
ASTM D-790 | 1100 kg/cm2 |
Electrical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Volume resistivity | JIS K-6911 | >1016 | |
Dielectric loss | MF|0.05 | ||
0.05 | |||
Volume resistivity | JIS K-6911 | MF|>1015 | |
JIS K-6911 | >1015 | ||
arc resistance | JIS K-6911 | MF|没有痕迹 | |
JIS K-6911 | 没有痕迹 | ||
dielectric strength | MF|20 | ||
20 | |||
dielectric constant | MF|3.7 | ||
3.7 | |||
Volume resistivity | JIS K-6911 | MF|>1016 |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
specific heat | 0.35 cal/g/℃ | ||
Linear coefficient of thermal expansion | ASTM D-696 | MF|6×10-5 cm/cm/℃ | |
ASTM D-696 | 6×10-5 cm/cm/℃ | ||
Heat distortion temperature | ASTM D-648 | MF|82 °C | |
ASTM D-648 | 92 °C | ||
vicat | ASTM D-1525 | MF|97 °C | |
ASTM D-1525 | 107 °C | ||
thermal conductivity | ASTM C-177 | MF|5×10-4 Cal/s/cm/℃ | |
ASTM C-177 | 5×10-4 Cal/s/cm/℃ | ||
specific heat | MF|0.35 cal/g/℃ |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.