HDPE DOW™ DMDA-8007 DOW USA
269
- Unit Price:US$ 1,273 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:10MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:Resistance to stress cracking|High rigidity|High gloss
- Application Areas:--
- Color:--
- Grade:Injection grade
Technical Data Sheet
| Basic Performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| melt mass-flow rate | 190℃/2.16kg | ASTM D-1238 | 8.25 g/10min |
| density | ASTM D-792 | 0.965 g/cm³ | |
| melt mass-flow rate | 190℃/21.6kg | ASTM D-1238 | 180 g/10min |
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| elongation | Break | ASTM D-638 | 354 % |
| elongation at yield | ASTM D-638 | 6 % | |
| tensile strength | Break | ASTM D-638 | 2600(18) Psi(MPa) |
| Shore hardness | ASTM D-2240 | 61 Shore D | |
| Bending modulus | 2%割线 | ASTM D-790 B | 205.000(1413) Psi(MPa) |
| Impact strength of cantilever beam gap | ASTM D-1822 | 80(168) ft?lb/in2(kJ/m2) | |
| Environmental stress cracking resistance | 122?H(50℃),F50,100%lgepal | ASTM D-1693 | 2 hrs |
| tensile strength | Yield | ASTM D-638 | 4500(31) Psi(MPa) |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Melting temperature | DSC法 | Dow Method | 271(133) ℉(℃) |
| Hot deformation temperature | 66psi(0.45MPa) | ASTM D-648 | 183(84) ℉(℃) |
| Crystallization peak temperature | DSC法 | Dow Method | 248(120) ℉(℃) |
| Vicat softening temperature | ASTM D-1525 | 268(131) ℉(℃) | |
| Brittle temperature | ASTM D-746 | <-105(<-76) ℉(℃) |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.