Material Description
- Material Properties:Low temperature impact resistance|gas barrier
- Application Areas:Electrical applications|chip|Shell|sporting goods|Pneumatic applications|Industrial applications|Engineering accessories|Application in the automotive field|Power/Other Tools|Household goods|Laptop case|Hydraulic applications|Home appliance components|Medical devices|Consumer product application field
- Color:--
- Grade:Flame retardant enhanced grade
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of simply supported beam without notch | 23°C | kJ/m² | 90 | |
| -30°C | kJ/m² | 90 | ||
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| Flammability level | 0.8mm | HB | -- | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Tensile strain | Break | % | 5.0 | 6.0 |
| tensile strength | Break | 155 | MPa | |
| Tensile modulus | MPa | 12000 | 11500 | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Melting temperature | °C | 178 | -- | |
| Continuous use temperature | --4 | °C | 150 | -- |
| --3 | °C | 90.0to120 | -- | |
| Hot deformation temperature | 8.0MPa,Unannealed | °C | 125 | -- |
| 1.8MPa,Unannealed | °C | 165 | -- | |
| Linear coefficient of thermal expansion | TD | cm/cm/°C | 1.2E-04 | -- |
| MD | cm/cm/°C | 1.5E-05 | -- | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Water absorption rate | Equilibrium,23°C,50%RH | % | 0.40 | -- |
| Saturation,23°C | % | 0.80 | -- | |
| Shrinkage rate | MD | % | 0.10 | -- |
| TD | % | 0.50 | -- | |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Dielectric strength | kV/mm | -- | ||
| Volume resistivity | ohms·cm | -- | 1E+13 | |
| Surface resistivity | ohms | -- | 1E+12 | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Ball Pressure Test | MPa | 155 | -- | |
| Shore hardness | ShoreD,15Sec | 82 | -- |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.