Material Description
- Material Properties:High barrier|UV resistance
- Application Areas:Electronic and electrical accessories
- Color:--
- Grade:Injection grade
Technical Data Sheet
hardness | Test Condition | Test Method | Test Result |
---|---|---|---|
Shore hardness | ShoreA,30Sec | ASTM D2240 | 85 |
thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Hot deformation temperature | 121°C | CCP METHOD | 5.0 % |
Brittle temperature | ASTM D746 | <-40.0 °C |
flammability | Test Condition | Test Method | Test Result |
---|---|---|---|
Smoke density | Non-Flame,0.5mmplaque,Ds,max | ASTME662 | 47 |
Flame,0.5mmplaque,Ds,max | ASTME662 | 110 | |
VW | CCP METHOD | Pass | |
Extreme Oxygen Index | ISO 4589-2 | 27 % | |
Hot filament ignition temperature | 3.00mm | IEC 60695-2-13 | 825 °C |
Burning wire flammability index | 3.00mm | IEC 60695-2-12 | 850 °C |
Electrical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Compared to the anti leakage trace index | IEC 60112 | PLC 0 | |
Dissipation factor | 1MHz | ASTM D150 | 7E-03 |
Dielectric constant | 1MHz | ASTM D150 | 2.40 |
Dielectric strength | 2.00mm,in Oil | IEC 60243-1 | 25 KV/mm |
Volume resistivity | ASTM D257 | 1.9E+16 ohms·cm |
Physical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
melt mass-flow rate | 250°C/10.0kg | ASTM D1238 | 16 g/10min |
mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
crack | ASTM D638 | 16.0 Mpa | |
Fracture, 136 ° C | CCP METHOD | 22.0 Mpa | |
crack | ISO 527-2/50 | 16.0 Mpa | |
CCP METHOD | 23.0 Mpa | ||
100mm span | 100mm | ASTM D790 | 65.0 Mpa |
crack | ISO 527-2/50 | 250 % | |
Fracture, 136 ° C | CCP METHOD | 250 % | |
crack | ASTM D638 | 260 % | |
CCP METHOD | 310 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.