PPO NORYL GTX™ GTX979 BK SABIC INNOVATIVE US
185
- Unit Price:US$ 4,791 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:25MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
For more details, please contact the supplier!
Material Description
- Material Properties:High mobility|dimensional stability |High temperature resistance|Hydrolysis resistance
- Application Areas:Electrical applications|Industrial machinery|Application in the automotive field
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
melt mass-flow rate | ASTM D1238 | 15 g/10min | |
Melt volume flow rate | ISO 1133 | 11.0 cm3/10min | |
Shrinkage rate | 内部方法 | 1.2-1.6 % | |
内部方法 | 1.2-1.6 % | ||
Water absorption rate | ISO 62 | 4.2 % | |
ISO 62 | 1.2 % |
flammability | Test Condition | Test Method | Test Result |
---|---|---|---|
Burning wire flammability index | IEC 60695-2-12 | 650 °C |
Impact resistance | Test Condition | Test Method | Test Result |
---|---|---|---|
Charpy Notched Impact Strength | ISO 179/1eA | 12 kJ/m² | |
ISO 179/1eA | 20 kJ/m² | ||
Suspended wall beam without notch impact strength | ISO 180/1U | 无断裂 | |
ISO 180/1U | 无断裂 | ||
Dart impact | ASTM D3763 | 50.0 J |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
tensile strength | ASTM D638 | 50.0 Mpa | |
ISO 527-2/50 | 50.0 Mpa | ||
elongation | ASTM D638 | 5.0 % | |
ISO 527-2/50 | 4.0 % | ||
ASTM D638 | 60 % | ||
ISO 527-2/50 | 30 % | ||
Flexural modulus | ASTM D790 | 2050 Mpa | |
ISO 178 | 2150 Mpa | ||
bending strength | ISO 178 | 80.0 Mpa | |
ASTM D790 | 80.0 Mpa | ||
Tensile modulus | ASTM D638 | 2000 Mpa | |
ISO 527-2/1 | 2100 Mpa | ||
tensile strength | ASTM D638 | 55.0 Mpa | |
ISO 527-2/50 | 55.0 Mpa |
Electrical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Volume resistivity | 内部方法 | 1.0E+3-1.0E+4 ohms·cm |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Heat distortion temperature | ISO 75-2/Be | 178 °C | |
vicat | ASTMD152511 | 180 °C | |
ISO 306/B120 | 182 °C | ||
Linear coefficient of thermal expansion | ASTME831 | 9.5E-05 cm/cm/°C | |
ISO 11359-2 | 9.6E-05 cm/cm/°C | ||
ASTME831 | 1E-04 cm/cm/°C | ||
ISO 11359-2 | 9.6E-05 cm/cm/°C | ||
Heat distortion temperature | ASTM D648 | 185 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.