Material Description
- Material Properties:Hydrolysis resistance|High temperature resistance|Dimensional stability|High mobility|Filler: Glass fiber reinforced material
- Application Areas:Industrial machinery|Electrical applications
- Color:--
- Grade:--
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 8.0 kJ/m² |
| Impact strength of cantilever beam gap | -30°C | ISO 180/1A | 6.0 kJ/m² |
| 23°C | ISO 180/1A | 7.0 kJ/m² |
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Tensile modulus | ISO 527-2/1 | 6800 Mpa | |
| tensile strength | Yield | ISO 527-2/5 | 125 Mpa |
| Break | ISO 527-2/5 | 125 Mpa | |
| Tensile strain | Yield | ISO 527-2/5 | 3.0 % |
| Break | ISO 527-2/5 | 3.5 % | |
| Bending modulus | ISO 178 | 5000 Mpa | |
| bending strength | ISO 178 | 175 Mpa |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Hot deformation temperature | 0.45MPa,Unannealed,64.0mmSpan | ISO 75-2/Bf | 240 °C |
| Vicat softening temperature | ISO 306/B50 | 235 °C | |
| Linear coefficient of thermal expansion | MD:23to60°C | ISO 11359-2 | 3.5E-05 cm/cm/°C |
| TD:23to60°C | ISO 11359-2 | 7.5E-05 cm/cm/°C |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Melt Volume Flow Rate (MVR) | 280°C/10.0kg | ISO 1133 | 4.00 cm3/10min |
| Water absorption rate | Saturation,23°C | ISO 62 | 2.5 % |
| Equilibrium,23°C,50%RH | ISO 62 | 1.0 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.