MVLDPE Exceed™ 1018CA EXXONMOBIL USA
396
- Unit Price:US$ 1,144 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:20MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:High impact resistance|high strength
- Application Areas:Shipping container|chip|film
- Color:--
- Grade:Thin film grade
Technical Data Sheet
| optical performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| turbidity | ASTM D-1003 | 18 % | |
| gloss | Across Flow,45° | ASTM D-2457 | 42 |
| 45° | ASTM D2457 | 39 | |
| turbidity | ASTM D1003 | 18 % |
| Other performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| PPA | 有 | ||
| Anti adhesive agent | 否 | ||
| Slippery agent | 否 | ||
| thermal stability | 有 |
| Basic Performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| melt mass-flow rate | ASTM D-1238 | 1 g/10min | |
| density | ExxonMobil Method | 0.918 g/cm³ |
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| tensile strength | @厚 150μ(5.9mil),MD | ASTM D-882 | 9 Mpa |
| @厚 150μ(5.9mil),TD,Yield | ASTM D-882 | 9.7 Mpa | |
| @厚 150μ(5.9mil),MD | ASTM D-882 | 75.8 Mpa | |
| @厚 150μ(5.9mil),TD | ASTM D-882 | 62.7 Mpa | |
| Elongation at Break | @厚 150μ(5.9mil),MD | ASTM D-882 | 500 % |
| @厚 150μ(5.9mil),TD | ASTM D-882 | 700 % | |
| Secant modulus | @厚 150μ(5.9mil),1%Strain, MD | ASTM D-882 | 183 Mpa |
| @厚 150μ(5.9mil),1%Strain, TD | ASTM D-882 | 205 Mpa | |
| Dart impact | F50 | ASTM D-1709A | 560 g |
| Elmendorf tear strength | MD | ASTM D-1922 | 280 g |
| TD | ASTM D-1922 | 460 g | |
| Puncture resistance | ExxonMobil Method | 4.3 J |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Melt Temperature | ExxonMobil Method | 119 °C |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| melt mass-flow rate | 190°C/2.16kg | ASTM D1238 | 1.0 g/10min |
| film | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Secant modulus -1% Decant, MD | ASTM D882 | 185 Mpa | |
| Secant modulus -1% Decant, TD | ASTM D882 | 192 Mpa | |
| tensile strength | Yield | ASTM D882 | 9.37 Mpa |
| Yield | ASTM D882 | 9.40 Mpa | |
| Break | ASTM D882 | 54.3 Mpa | |
| Break,TD | ASTM D882 | 42.7 Mpa | |
| elongation | Break | ASTM D882 | 500 % |
| Tensile strain | Break | ASTM D882 | 600 % |
| Dart impact | ASTM D1709A | 460 g | |
| Elmendorf tear strength | MD | ASTM D1922 | 250 g |
| TD | ASTM D1922 | 470 g |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.