Material Description
- Material Properties:Thermal stability
- Application Areas:--
- Color:--
- Grade:--
Technical Data Sheet
thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Heat Deflection Temperature | 0.45 MPa,Unannealed 66 psi, Unannealed | ISO 75-2/B | 114 °C |
1.8 MPa,Unannealed 264 psi, Unannealed | ISO 75-2/A | 46 °C | |
Glass Transition Temperature | ISO 11357-2 | -43 °C | |
vicat | B50B50 | ISO 306 | 107 °C |
melting temperature | ISO 11357-3 | 158 °C | |
Linear coefficient of thermal expansion | MDMD | ISO 11359-2 | 0.00016 1/℃ |
flame retardant performance | Test Condition | Test Method | Test Result |
---|---|---|---|
UL flame retardant rating | UL 94 | V-0 | |
Limiting Oxygen Index | ISO 4589-2 | 43 % |
Physical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Melt volume flow rate | 230℃,5 kg230℃/5.0 kg | ISO 1133 | 1.1 cm3/10min |
Water absorption rate | Saturation,23℃ Saturation, 73°F | ISO 62 | 0.03 % |
Equilibrium,23℃,50% RH Equilibrium, 73°F, 50% RH | ISO 62 | 0.015 % |
Electrical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Surface Resistivity | IEC 60093 | 10000000000000 ohms | |
volume resistivity | IEC 60093 | 200000000000000 ohms·cm | |
dielectric strength | IEC 60243-1 | 21 KV/mm | |
relative permittivity | 100 Hz100 Hz | IEC 60250 | 10.5 |
1 MHz1 MHz | IEC 60250 | 6.5 | |
Dissipation Factor | 100 Hz100 Hz | IEC 60250 | 0.038 |
1 MHz1 MHz | IEC 60250 | 0.23 | |
Compared to the Leakage Tracking Index (CTI) | IEC 60112 | V |
mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile modulus | ISO 527-2 | 1300 Mpa | |
tensile strength | Yield Yield | ISO 527-2 | 40 Mpa |
Tensile strain | Yield Yield | ISO 527-2 | 11 % |
Nominal tensile fracture strain | ISO 527-2 | > 50 % | |
Tensile creep modulus | 1 hr1 hr | ISO 899-1 | 508 Mpa |
1000 hr1000 hr | ISO 899-1 | 210 Mpa |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.