PA66 GP2130BW NP LG GUANGZHOU

210
  • Unit Price:US$ 3,496 /MT
  • Packaging Specification:
    25 KG/PKG
  • Packaging Material:
    Paper bag
  • Supply Quantity:
    25MT
  • Delivery Terms:
    FOB
  • Port of Loading :
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 ********View
serv********View

For more details, please contact the supplier!

Material Description

  • Material Properties:--
  • Application Areas:--
  • Color:--
  • Grade:--

Technical Data Sheet Compare

hardnessTest ConditionTest MethodTest Result
Rockwell hardnessR 级, 23°C, 注塑ASTM D785121
thermal performanceTest ConditionTest MethodTest Result
Heat Deflection Temperature0.45 MPa, 未退火, 6.40 mm, 注塑ASTM D648255 °C
Heat Deflection Temperature1.8 MPa, 未退火, 6.40 mm, 注塑ASTM D648240 °C
melting temperatureASTM D3418260 °C
Linear coefficient of thermal expansion流动ASTM D6964.0E-5 cm/cm/°C
RTI Elec0.75 mmUL 746120 °C
RTI Elec1.5 mmUL 746110 °C
RTI Elec3.0 mmUL 746120 °C
RTI Imp0.75 mmUL 746120 °C
RTI Imp1.5 mmUL 746110 °C
RTI Imp3.0 mmUL 746120 °C
RTI0.75 mmUL 746120 °C
RTI1.5 mmUL 746110 °C
RTI3.0 mmUL 746120 °C
flammabilityTest ConditionTest MethodTest Result
UL flame retardant rating0.75 mmUL 94HB
UL flame retardant rating1.5 mmUL 94HB
UL flame retardant rating3.0 mmUL 94HB
Physical propertiesTest ConditionTest MethodTest Result
shrinkage rate23°C, 3.20 mm, 注塑,FlowASTM D9550.70 - 1.2 %
Water absorption rate24 hr, 23°CASTM D5701.0 %
Electrical performanceTest ConditionTest MethodTest Result
volume resistivity23°CASTM D2571.0E+16 ohms·cm
dielectric strength23°C, 1.00 mmASTM D14925 KV/mm
dielectric constant23°C, 1 MHzASTM D1504.00
injectionTest ConditionTest MethodTest Result
drying temperature80 to 100 °C
drying time4.0 to 5.0 hr
Temperature at the rear of the barrel265 to 275 °C
Temperature in the middle of the barrel270 to 280 °C
Temperature at the front of the material cylinder270 to 285 °C
Spray nozzle temperature270 to 280 °C
Processing (melt) temperature270 to 290 °C
mold temperature80 to 110 °C
Back pressure29.4 to 58.8 Mpa
screw speed30 to 60 rpm
mechanical propertiesTest ConditionTest MethodTest Result
tensile strength断裂, 23°C, 3.20 mm, 注塑ASTM D638123 Mpa
elongation断裂, 23°C, 3.20 mm, 注塑ASTM D6384.0 %
flexural modulus23°C, 3.20 mm, 注塑ASTM D7904900 Mpa
bending strength23°C, 3.20 mm, 注塑ASTM D790167 Mpa
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.