PPO XYRON™ X352H BK ASAHI JAPAN
267
- Unit Price:US$ 3,998 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:10MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:Chemical resistance|Low temperature resistance|Filler: Filler|20% filler by weight
- Application Areas:Fitness equipment|Sports Equipment
- Color:--
- Grade:Injection grade
Technical Data Sheet
impact performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Charpy Notched Impact Strength | 23°C | ISO 179 | 4.0 kJ/m² |
flammability | Test Condition | Test Method | Test Result |
---|---|---|---|
UL flame retardant rating | 1.5mm | UL 94 | HB |
mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
bending strength | 23°C | ISO 178 | 99.0 Mpa |
Bending modulus | 23°C | ISO 178 | 4700 Mpa |
Tensile strain | Break,23°C | ISO 527-2 | 10 % |
tensile strength | Yield,23°C | ISO 527-2 | 50.0 Mpa |
thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Linear coefficient of thermal expansion | MD:-30to65°C | ISO 11359-2 | 5E-05 cm/cm/°C |
Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 97.0 °C |
1.8MPa,Unannealed | ASTM D648 | 100 °C |
Physical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Water absorption rate | 23°C,24hr | ISO 62 | 0.060 % |
Shrinkage rate | 2.00mm | Internal Method | 0.35-0.55 % |
Electrical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Volume resistivity | 23°C | IEC 60093 | 1E+16 ohms·cm |
Surface resistivity | IEC 60093 | 1E+16 ohms |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.