Material Description
- Material Properties:currency|Medium viscosity|Medium viscosity|For general injection molding
- Application Areas:Industrial applications|Electrical field|Electronic field|Automotive sector|Used for industrial accessories|Automotive electronic components|Electronic and electrical accessories; ul certification
- Color:--
- Grade:--
Technical Data Sheet
other | Test Condition | Test Method | Test Result |
---|---|---|---|
Water absorption rate | ISO 62 | 0.30 % | |
density | ISO 1183 | 1200 kg/m2 | |
Water absorption rate | ISO 62 | 0.12 % |
thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Glow wire ignition temperature (GWIT) | IEC 60695-2-13 | 875 ℃ | |
IEC 60695-2-13 | 875 ℃ | ||
Glow wire combustion index (GWFI) | IEC 60695-2-12 | 930 ℃ | |
IEC 60695-2-12 | 850 ℃ | ||
Limiting Oxygen Index | ISO 4589-2 | 27 % | |
UL flame retardant rating | UL 94 | 级 | |
UL 94 | HB(2.5) 级 | ||
UL 94 | V-2 级 | ||
Linear coefficient of thermal expansion | ISO 11359-1-2 | 0.65 10-4/K | |
ISO 11359-1-2 | 0.65 10-4/K | ||
vicat | ISO 306 | 145 ℃ | |
Glass Transition Temperature | ISO 11357-1-2 | 145 ℃ |
Specific properties of raw materials | Test Condition | Test Method | Test Result |
---|---|---|---|
transmittance | ISO 13468-2 | 89 % | |
refractive index | ISO 489 | 1.586 -- |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Elongation at break | ISO 527-1-2 | >50 % | |
Tensile strain | ISO 527-1-2 | 6.1 % | |
Tensile creep modulus | ISO 899-1 | 2200 MPa | |
fracture strain | ISO 527-1-2 | -- % | |
Tensile modulus | ISO 527-1-2 | 2400 MPa | |
Tensile stress | ISO 527-1-2 | 66 MPa | |
tensile strength | ISO 6603-2 | 60 J | |
Maximum destructive power | ISO 6603-2 | 5400 N | |
Impact strength of cantilever beam gap | kJ/m² | 参照ISO 180/1eA 85P(C) | |
Charpy Notched Impact Strength | kJ/m² | 参照ISO 179/1eA 75P(C) | |
ISO 179/1eU | N kJ/m² | ||
flexural modulus | ISO 179 | 2400 MPa | |
Tensile creep modulus | ISO 899-1 | 1900 MPa | |
Breaking stress | ISO 527-1-2 | -- MPa |
Physical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
melt mass-flow rate | ISO 1133 | -- cm3/(10分钟) | |
ISO 1133 | 9.5 cm3/(10分钟) | ||
shrinkage rate | ISO 294-4 | 0.65 % | |
ISO 294-4 | 0.7 % |
Electrical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Compared to the Leakage Traceability Index (CTI) | IEC 60112 | 250 等级 | |
dielectric strength | IEC 60243-1 | 34 kv/毫米 | |
Surface Resistivity | IEC 60093 | 1E+16 Ohm | |
volume resistivity | IEC 60093 | 1E+14 Ohm.m | |
Dissipation Factor | IEC 60250 | 90 10-4 | |
IEC 60250 | 5 10-4 | ||
dielectric constant | IEC 60250 | 3.0 -- | |
IEC 60250 | 3.1 -- |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.