PC/ABS CYCOLOY™  C2950-111 SABIC INNOVATIVE NANSHA

316
Unit Price:$2711 USD/MT
Packaging Specification:
25 KG/PKG
Supply Quantity:
438.5MT
Delivery Terms:
FOB
Port of Loading:
China Main Port
Accepted Payment Methods:
T/T
Shipping:
Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 2787 3515View
serv********View

For more detailed information including pricing, customization, and shipping, please contact supplier.

Material Description
Technical Data Sheet

Material Description

  • Material Properties:Flame retardant High mobility High impact resistance High temperature resistan heat-resisting
  • Application Areas:Electrical field Electronic field Household appliances Household appliances Automotive sector
  • Color:--
  • Grade:Injection grade

Technical Data Sheet Compare

physical propertyTest ConditionTest MethodTest ResultUnit
Melt mass flow rate260°C/2.16kgASTMD123810g/10min
Shrinkage rateMD:3.20mm内部方法0.40to0.60%
Shrinkage rateTD:3.20mm内部方法0.40to0.60%
Water absorption rate24hrASTMD5700.10%
Water absorption rateEquilibrium,23°CASTMD5700.40%
density--ASTMD7921.18g/cm³
density--2ASTMD7921.22g/cm³
Mechanical performanceTest ConditionTest MethodTest ResultUnit
Impact strength of cantilever beam gap23°CASTMD256530J/m
Dart impact equipped with measuring instruments-30°C,TotalEnergyASTMD376354.2J
Dart impact equipped with measuring instruments23°C,TotalEnergyASTMD376361.0J
Rockwell hardnessR-ScaleASTMD785123
tensile strengthYieldASTMD63862.7Mpa
elongationBreakASTMD63840%
Bending modulus100mmSpanASTMD7902650Mpa
Flexural StrengthYield,100mmSpanASTMD790102Mpa
Impact strength of cantilever beam gap-30°CASTMD256160J/m
Thermal performanceTest ConditionTest MethodTest ResultUnit
thermal conductivityASTMC1770.20W/m/K
RTIElecUL74685.0°C
RTI ImpUL74685.0°C
RTIStrUL74685.0°C
Hot deformation temperature0.45MPa,Unannealed,6.40mmASTMD648104°C
Hot deformation temperature1.8MPa,Unannealed,3.20mmASTMD64890.6°C
Hot deformation temperature1.8MPa,Unannealed,6.40mmASTMD64895.0°C
vicat softening pointASTMD15255113°C
Linear coefficient of thermal expansionMD:-30to30°CASTMD6967.2E-05cm/cm/°C
Linear coefficient of thermal expansionTD:-30to30°CASTMD6967.2E-05cm/cm/°C
Electrical performanceTest ConditionTest MethodTest ResultUnit
Dissipation factor50HzASTMD1505E-03
Dissipation factor60HzASTMD1505E-03
Dissipation factor100HzASTMD1504.9E-03
Arc resistanceASTMD495PLC6
Compared to the anti leakage trace indexCTIUL746PLC1
High arc combustion indexHAIUL746PLC0
High voltage arc tracing rateHVTRUL746PLC2
Hot wire ignitionHWIUL746PLC1
Surface resistivityASTMD257>1.0E+16ohms
Volume resistivityASTMD2571E+17ohms·cm
Dielectric strength3.20mm,inOilASTMD14919KV/mm
Dielectric constant50HzASTMD1503.00
Dielectric constant60HzASTMD1503.00
Dielectric constant100HzASTMD1503.00
flammabilityTest ConditionTest MethodTest ResultUnit
Extreme Oxygen IndexASTMD286332%
UL flame retardant rating1.5mmUL94V-0
UL flame retardant rating2.5mmUL945VB
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.