PC LUPOY® 1201-10 LG CHEM KOREA
281
Unit Price:$2013 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 298MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:transparent wear resistant Food contact compliance Medium viscosity Good demolding performanc
- Application Areas:Toy Food packaging chip container chip Disposable tableware Toy
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
density | ASTMD792 | 1.20 | g/cm³ | |
Melt mass flow rate | 300°C/1.2kg | ASTMD1238 | 10 | g/10min |
Shrinkage rate | MD | ASTMD955 | 0.50到0.70 | % |
Water absorption rate | 23°C,24hr | ASTMD570 | 0.15 | % |
Equilibrium,23°C,50%RH | ASTMD570 | 0.32 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell hardness | M-Scale | ASTMD785 | 73 | |
R-Scale | ASTMD785 | 118 | ||
Tensile modulus | ASTMD638 | 2410 | Mpa | |
tensile strength | Yield,23°C1 | ASTMD638 | 60.0 | Mpa |
Break | ASTMD638 | 71.0 | Mpa | |
elongation | Yield | ASTMD638 | 6.0 | % |
Break | ASTMD638 | 150 | % | |
Bending modulus | ASTMD790 | 2410 | Mpa | |
bending strength | ASTMD790 | 96.0 | Mpa | |
Wear resistance - AngelinHaze | ASTMD1004 | 45 | % | |
Suspended wall beam gap impact strength | 23°C,3.20mm | ASTMD256 | 900 | J/m |
Cantilever beam without notch impact strength | 23°C | ASTMD256 | 无断裂 | |
Dart impact equipped with measuring instruments | 23°C,3.20mm,TotalEnergy | ASTMD3763 | 87.0 | J |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hot deformation temperature | 0.45MPa,Annealed,4.00mm | ASTMD648 | 144 | °C |
1.8MPa,Unannealed,4.00mm | ASTMD648 | 128 | °C | |
1.8MPa,Annealed,4.00mm | ASTMD648 | 141 | °C | |
vicat softening point | ASTMD15255 | 149 | °C | |
Ball pressure temperature | IEC60598-1 | >125 | °C | |
Linear coefficient of thermal expansion | MD:-40to82°C | ASTMD696 | 6.8E-05 | cm/cm/°C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Volume resistivity | 23°C | ASTMD257 | 2E+17 | ohms·cm |
Dielectric strength | ASTMD149 | 17 | KV/mm | |
Dielectric constant | 60Hz | ASTMD150 | 3.00 | |
Dissipation factor | 60Hz | ASTMD150 | 1E-03 | |
Leakage Trace Index | 2.00mm | IEC60112 | 250 | V |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Refractive index | ASTMD542 | 1.586 | ||
Light transmittance | ASTMD1003 | 89.0 | % | |
Haze | ASTMD1003 | 0.70到1.5 | % |
flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL flame retardant rating | 3.00mm | UL94 | HB | |
0.500mm | UL94 | V-2 | ||
1.60mm | UL94 | V-2 | ||
2.50mm | UL94 | V-2 | ||
2.70mm | UL94 | V-2 | ||
Hot filament ignition temperature | 2.00mm | IEC60695-2-13 | 850 | °C |
Extreme Oxygen Index | ASTMD2863 | 26 | % | |
Average degree of combustion | ASTMD635 | 3 | CM |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.