POM Delrin® 525GR NC000 DUPONT USA
324
- Unit Price:US$ 8,394 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:77MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:enhance|wear resistant|Medium viscosity|High rigidity|high strength|Filler: Glass fiber reinforced material|25% filler by weight
- Application Areas:Household appliances|Fitness equipment|Automotive sector
- Color:--
- Grade:Injection grade
Material Certification

Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Impact strength of simply supported beam without notch | -30°C | ISO 179/1eU | 50 kJ/m² |
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 10 kJ/m² |
| -30°C | ISO 179/1eA | 10 kJ/m² | |
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 60 kJ/m² |
| flammability | Test Condition | Test Method | Test Result |
|---|---|---|---|
| FMVSS flammability | FMVSS302 | B | |
| Fogging-G-value | condensate | ISO 6452 | 1.2 mg |
| UL flame retardant rating | 1.5mm | IEC 60695-11-10,-20 | HB |
| 0.75mm | IEC 60695-11-10,-20 | HB | |
| 1.5mm | UL 94 | HB | |
| 0.75mm | UL 94 | HB | |
| Burning rate | 1.00mm | ISO 3795 | 49 mm/min |
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Tensile modulus | ISO 527-2 | 9500 Mpa | |
| tensile strength | Break | ISO 527-2 | 160 Mpa |
| Tensile strain | Break | ISO 527-2 | 3.0 % |
| Tensile creep modulus | 1hr | ISO 899-1 | 8500 Mpa |
| 1000hr | ISO 899-1 | 6000 Mpa |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| AnnealingTemperature | 160 °C | ||
| Linear coefficient of thermal expansion | TD | ISO 11359-2 | 1E-04 cm/cm/°C |
| MD | ISO 11359-2 | 3.5E-05 cm/cm/°C | |
| AnnealingTime-Optional | 30.0 min/mm | ||
| Melting temperature | ISO 11357-3 | 178 °C | |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 172 °C |
| 0.45MPa,Unannealed | ISO 75-2/B | 176 °C |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Water absorption rate | Saturation,23°C,2.00mm | ISO 62 | 1.3 % |
| Shrinkage rate | MD | ISO 294-4 | 0.40 % |
| TD | ISO 294-4 | 1.2 % | |
| Melt Volume Flow Rate (MVR) | 190°C/2.16kg | ISO 1133 | 5.00 cm3/10min |
| density | ISO 1183 | 1.60 g/cm³ | |
| Water absorption rate | Equilibrium,23°C,2.00mm,50%RH | ISO 62 | 0.17 % |
| Electrical performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Relative permittivity | 1MHz | IEC 60250 | 3.80 |
| 100Hz | IEC 60250 | 3.70 | |
| Volume resistivity | IEC 60093 | 1E+14 ohms·cm |
| Supplementary Information | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Emission | VDA275 | <8.00 mg/kg | |
| EmissionofOrganicCompounds | VDA277 | 5.00 µgC/g |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.