ABS ECO GP-22 MR70 INEOS STYRO KOREA
200
Unit Price:$2105 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Impact resistance Heat resistant deformatio
- Application Areas:Electrical enclosure Household appliances electronic product
- Color:--
- Grade:--
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Water absorption rate | Equilibrium,23°C,50%RH | ISO62 | 0.22 | % |
density | ASTMD792 | 1.04 | g/cm³ | |
ISO1183 | 1.04 | g/cm³ | ||
Melt mass flow rate | 200°C/5.0kg | ASTMD1238 | 1.5 | g/10min |
220°C/10.0kg | ASTMD1238 | 19 | g/10min | |
Melt Volume-Flow Rate (MVR) | 230°C/3.8kg | ASTMD1238 | 4.80 | cm3/10min |
220°C/10.0kg | ISO1133 | 19.0 | cm3/10min | |
Shrinkage rate | MD | ASTMD955 | 0.40to0.70 | % |
ISO294-4 | 0.40to0.70 | % | ||
Water absorption rate | Saturation,23°C | ASTMD570 | 1.0 | % |
Saturation,23°C | ISO62 | 1.0 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile modulus | ASTMD638 | 2300 | Mpa | |
ISO527-2 | 2300 | Mpa | ||
tensile strength | Yield,23°C | ASTMD638 | 45.0 | Mpa |
Yield,23°C | ISO527-2 | 45.0 | Mpa | |
elongation | Yield,23°C | ISO527-2 | 2.6 | % |
Break | ASTMD638 | 2.6 | % | |
Nominal tensile fracture strain | 23°C | ISO527-2 | 10 | % |
Bending modulus | ASTMD790 | 2300 | Mpa | |
bending strength | ASTMD790 | 65.0 | Mpa | |
ISO178 | 65.0 | Mpa | ||
Charpy Notched Impact Strength | -30°C | ISO179 | 8.0 | kJ/m² |
23°C | ISO179 | 22 | kJ/m² | |
Impact strength of simply supported beam without notch | -30°C | ISO179 | 100 | kJ/m² |
23°C | ISO179 | 180 | kJ/m² | |
Impact strength of cantilever beam gap | -30°C | ASTMD256 | 59 | J/m |
-18°C | ASTMD256 | 100 | J/m | |
23°C | ASTMD256 | 300 | J/m | |
-30°C | ISO180/A | 8.0 | kJ/m² | |
23°C | ISO180/A | 26 | kJ/m² | |
Rockwell hardness | R-Scale | ASTMD785 | 103 | |
Ball pressure hardness | ISO2039-1 | 97.0 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hot deformation temperature | 0.45MPa,Unannealed | ASTMD648 | 90.6 | °C |
0.45MPa,Annealed | ASTMD648 | 104 | °C | |
0.45MPa,Annealed | ISO75-2/B | 99.0 | °C | |
1.8MPa,Unannealed | ASTMD648 | 77.8 | °C | |
1.8MPa,Annealed | ASTMD648 | 98.9 | °C | |
1.8MPa,Annealed | ISO75-2/A | 94.0 | °C | |
vicat softening point | -- | ISO306/A50 | 105 | °C |
-- | ISO306/B50 | 96.0 | °C | |
Linear coefficient of thermal expansion | MD | ISO11359-2 | 8.0E-5to1.1E-4 | cm/cm/°C |
thermal conductivity | DIN52612 | 0.17 | W/m/K |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Surface resistivity | IEC60093 | 1E+13 | ohms | |
Volume resistivity | ASTMD257 | >1.0E+15 | ohms·cm | |
IEC60093 | 1E+15 | ohms·cm | ||
Dielectric constant | 1.00mm,1MHz | ASTMD150 | 2.80 | |
Relative permittivity | 100Hz | IEC60250 | 2.90 | |
1MHz | IEC60250 | 2.80 | ||
Dissipation factor | 100Hz | IEC60250 | 4.8E-03 | |
1MHz | IEC60250 | 7.9E-03 |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Huangdu Index | DIN6167 | 13 | YI |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.
Contact Us
Get App
Top