ABS Terluran® GP-22 INEOS STYRO KOREA
248
Unit Price:$1723 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 67MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:High mobility
- Application Areas:Electronic communication small home appliances
- Color:--
- Grade:Injection grade
Technical Data Sheet
物理性能 | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
吸水率 | 平衡,23°C,50%RH | ISO62 | 0.22 | % |
密度 | ASTMD792 | 1.04 | g/cm³ | |
ISO1183 | 1.04 | g/cm³ | ||
熔体质量流动速率 | 200°C/5.0kg | ASTMD1238 | 1.5 | g/10min |
220°C/10.0kg | ASTMD1238 | 19 | g/10min | |
熔体体积流动速率 | 230°C/3.8kg | ASTMD1238 | 4.80 | cm3/10min |
220°C/10.0kg | ISO1133 | 19.0 | cm3/10min | |
收缩率 | MD | ASTMD955 | 0.40to0.70 | % |
ISO294-4 | 0.40to0.70 | % | ||
吸水率 | 饱和,23°C | ASTMD570 | 1.0 | % |
饱和,23°C | ISO62 | 1.0 | % |
机械性能 | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
拉伸模量 | ASTMD638 | 2300 | Mpa | |
ISO527-2 | 2300 | Mpa | ||
拉伸强度 | 屈服,23°C | ASTMD638 | 45.0 | Mpa |
屈服,23°C | ISO527-2 | 45.0 | Mpa | |
伸长率 | 屈服,23°C | ISO527-2 | 2.6 | % |
断裂 | ASTMD638 | 2.6 | % | |
标称拉伸断裂应变 | 23°C | ISO527-2 | 10 | % |
弯曲模量 | ASTMD790 | 2300 | Mpa | |
弯曲强度 | ASTMD790 | 65.0 | Mpa | |
ISO178 | 65.0 | Mpa | ||
简支梁缺口冲击强度 | -30°C | ISO179 | 8.0 | kJ/m² |
23°C | ISO179 | 22 | kJ/m² | |
简支梁无缺口冲击强度 | -30°C | ISO179 | 100 | kJ/m² |
23°C | ISO179 | 180 | kJ/m² | |
悬壁梁缺口冲击强度 | -30°C | ASTMD256 | 59 | J/m |
-18°C | ASTMD256 | 100 | J/m | |
23°C | ASTMD256 | 300 | J/m | |
-30°C | ISO180/A | 8.0 | kJ/m² | |
23°C | ISO180/A | 26 | kJ/m² | |
洛氏硬度 | R级 | ASTMD785 | 103 | |
球压硬度 | ISO2039-1 | 97.0 | Mpa |
热性能 | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
热变形温度 | 0.45MPa,未退火 | ASTMD648 | 90.6 | °C |
0.45MPa,退火 | ASTMD648 | 104 | °C | |
0.45MPa,Annealed | ISO75-2/B | 99.0 | °C | |
1.8MPa,未退火 | ASTMD648 | 77.8 | °C | |
1.8MPa,退火 | ASTMD648 | 98.9 | °C | |
1.8MPa,退火 | ISO75-2/A | 94.0 | °C | |
维卡软化点 | -- | ISO306/A50 | 105 | °C |
-- | ISO306/B50 | 96.0 | °C | |
线性热膨胀系数 | MD | ISO11359-2 | 8.0E-5to1.1E-4 | cm/cm/°C |
导热系数 | DIN52612 | 0.17 | W/m/K |
电气性能 | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
表面电阻率 | IEC60093 | 1E+13 | ohms | |
体积电阻率 | ASTMD257 | >1.0E+15 | ohms·cm | |
IEC60093 | 1E+15 | ohms·cm | ||
介电常数 | 1.00mm,1MHz | ASTMD150 | 2.80 | |
相对电容率 | 100Hz | IEC60250 | 2.90 | |
1MHz | IEC60250 | 2.80 | ||
耗散因数 | 100Hz | IEC60250 | 4.8E-03 | |
1MHz | IEC60250 | 7.9E-03 |
光学性能 | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
黄度指数 | DIN6167 | 13 | YI |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.