Material Description
Technical Data Sheet
Material Description
- Material Properties:High mobility|Impact resistance
- Application Areas:Electrical appliances|Electronic field|Electrical field
- Color:--
- Grade:High liquidity level
Technical Data Sheet
Physical | Test Condition | Test Method | Test Result |
---|---|---|---|
Density / Specific Gravity | ASTMD792 | 1.05 g/cm³ | |
ISO1183 | 1.04 g/cm³ | ||
Melt Mass-Flow Rate | 220°C/10.0kg | ISO1133 | 40 g/10min |
Modeling Shrinkage | MD | ASTMD955 | 0.40to0.60 % |
Moisture Absorption | 23°C,24hr | ASTMD570 | 0.30 % |
Thermal Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Heat Deflection Temperature | 1.8MPa,未退火,6.40mm | ASTMD648 | 86.0 °C |
1.8MPa,未退火,12.7mm | ASTMD648 | 92.0 °C | |
1.8MPa,未退火 | ISO75-2/A | 81.0 °C | |
Linear thermal expansion coefficient | MD | ASTMD696 | 7.2E-05 cm/cm/°C |
Thermal Conductivity | ASTMC177 | 0.16 W/m/K |
Flammability | Test Condition | Test Method | Test Result |
---|---|---|---|
Flame Rating | UL94 | HB |
Electrical Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Surface Resistivity | ASTMD257 | >1.0E+16 ohms | |
Volume Resistivity | 23°C | ASTMD257 | >1.0E+16 ohms·cm |
Dielectric Strength | ASTMD149 | 23 KV/mm | |
Dielectric Constant | 1kHz | ASTMD150 | 3.10 |
Dissipation Factor? | 1kHz | ASTMD150 | 6.2E-03 |
Mechanical Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Flexural Modulus | ASTMD790 | 2300 Mpa | |
Flexural Strength | ASTMD790 | 73.0 Mpa | |
Flexural Stress | ISO178 | 77.0 Mpa | |
Tensile Modulus | ISO527-2/1 | 2600 Mpa | |
Tensile Strength | 屈服 | ASTMD638 | 46.0 Mpa |
Tensile Stress | 屈服 | ISO527-2/50 | 51.0 Mpa |
Tensile Elongation | 断裂 | ASTMD638 | 15 % |
Tensile Strain | 断裂 | ISO527-2/50 | >10 % |
Hardness | Test Condition | Test Method | Test Result |
---|---|---|---|
Rockwell Hardness | R级 | ASTMD785 | 114 |
Impact Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Charpy Notched Impact Strength | 23°C | ISO179/1eA | 18 kJ/m² |
Notched Izod Impact Strength | -30°C,3.20mm | ASTMD256 | 110 J/m |
-30°C,12.7mm | ASTMD256 | 80 J/m | |
0°C,3.20mm | ASTMD256 | 160 J/m | |
0°C,12.7mm | ASTMD256 | 110 J/m | |
23°C,3.20mm | ASTMD256 | 220 J/m | |
23°C,12.7mm | ASTMD256 | 200 J/m |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.