POM/GF/PTFE LNP™ LUBRICOMP™  KFL4036 SABIC INNOVATIVE US

118
Unit Price:$4925 USD/MT
Packaging Specification:
25 KG/PKG
Supply Quantity:
10.3MT
Delivery Terms:
FOB
Port of Loading:
China Main Port
Accepted Payment Methods:
T/T
Shipping:
Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 2787 3515View
serv********View

For more detailed information including pricing, customization, and shipping, please contact supplier.

Material Description
Technical Data Sheet

Material Description

  • Material Properties:High temperature resistan UV resistance
  • Application Areas:Casters household electrical appl
  • Color:--
  • Grade:Injection grade

Technical Data Sheet Compare

physical propertyTest ConditionTest MethodTest ResultUnit
Shrinkage rateMD:24hrASTMD9550.70to1.0%
Shrinkage rateTD:24hrASTMD9551.0to3.0%
Water absorption rate24hr,50%RHASTMD5700.16%
Water absorption rateEquilibrium,23°C,50%RHISO620.26%
Mechanical performanceTest ConditionTest MethodTest ResultUnit
Tensile modulusASTMD63810800Mpa
Tensile modulusISO527-2/110600Mpa
Wear factor - WasherASTMD3702Modified23510^-10in^5-min/ft-lb-hr
Suspended wall beam notch impact strength23°CISO180/1A5.9kJ/m²
Unscented Izod Impact Strength23°CISO180/1U25kJ/m²
Dart impact equipped with measuring instruments23°C,TotalEnergyASTMD376310.3J
Multi axis Instrumented Impact EnergyISO6603-22.50J
tensile strengthBreakASTMD63888.0Mpa
tensile strengthBreakISO527-2/584.0Mpa
elongationBreakASTMD6381.3%
elongationBreakISO527-2/51.3%
Bending modulus50.0mmSpanASTMD7909280Mpa
Bending modulusISO1789930Mpa
bending strengthISO178130Mpa
bending strengthBreak,50.0mmSpanASTMD790107Mpa
friction coefficientDynamicASTMD3702Modified0.40
friction coefficientStaticASTMD3702Modified0.46
Thermal performanceTest ConditionTest MethodTest ResultUnit
Linear coefficient of thermal expansionMD:-30to30°CASTMD6969.5E-05cm/cm/°C
Linear coefficient of thermal expansionTD:-30to30°CASTMD6966.5E-05cm/cm/°C
Hot deformation temperature0.45MPa,Unannealed,3.20mmASTMD648183°C
Hot deformation temperature0.45MPa,Unannealed,64.0mmSpanISO75-2/Bf163°C
Hot deformation temperature1.8MPa,Unannealed,3.20mmASTMD648161°C
Hot deformation temperature1.8MPa,Unannealed,64.0mmSpanISO75-2/Af161°C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.