PC/CF LNP™ STAT-KON™ DC-1003 SABIC INNOVATIVE US
150
Unit Price:$5612 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Easy to form|Easy to demould|Filler: Carbon fiber rein
- Application Areas:Plastic bag|Electronic and Electrical
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical | Test Condition | Test Method | Test Result |
---|---|---|---|
Density / Specific Gravity | ISO1183,ASTMD792 | 1.24 g/cm³ | |
Flow:24hr | ASTMD955 | 0.040到0.10 % | |
ASTMD955 | 0.30到0.40 % | ||
Across Flow:24hr | ISO294-4 | 0.32到0.41 % | |
Flow:24hr | ISO294-4 | 0.040到0.13 % | |
ASTMD955 | 0.040到0.10 % | ||
ASTMD955 | 0.30到0.40 % | ||
Across Flow:24hr | ISO294-4 | 0.32到0.41 % | |
Flow:24hr | ISO294-4 | 0.040到0.13 % | |
Moisture Absorption | 24hr,50%RH | ASTMD570 | 0.16 % |
Thermal Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
0.45MPa, Unannealed,3.20mm | ASTMD648 | 145 °C | |
1.8MPa, Unannealed,3.20mm | ASTMD648 | 137 °C | |
1.8MPa, Unannealed,64.0mm Span | ISO75-2/Af | 146 °C | |
Linear thermal expansion coefficient | MD:-40到40°C | ASTME831,ISO11359-2 | 1.8E-05 cm/cm/°C |
TD:-40到40°C | ASTME831,ISO11359-2 | 5E-05 cm/cm/°C |
Mechanical Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
fracture | ASTMD638 | 2.1 % | |
ISO527-2 | 2.0 % | ||
--1 | ASTMD638 | 8780 Mpa | |
fracture | ASTMD638 | 110 Mpa | |
ISO527-2 | 109 Mpa | ||
ASTMD638 | 2.1 % | ||
ISO527-2 | 2.0 % | ||
--1 | ASTMD638 | 8780 Mpa | |
fracture | ASTMD638 | 110 Mpa | |
ISO527-2 | 109 Mpa |
Electrical Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Surface Resistivity | ASTMD257 | 10到1.0E+5 ohms | |
ASTMD257 | 10到1.0E+5 ohms |
Impact Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
23°C | ASTMD256 | 74 J/m | |
23°C2 | ISO180/1A | 6.4 kJ/m² | |
23°C | ASTMD4812 | 490 J/m | |
23°C3 | ISO180/1U | 33 kJ/m² | |
23°C | ASTMD256 | 74 J/m | |
23°C2 | ISO180/1A | 6.4 kJ/m² | |
23°C | ASTMD4812 | 490 J/m | |
23°C3 | ISO180/1U | 33 kJ/m² | |
23°C,EnergyatPeakLoad | ASTMD3763 | 15.5 J |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.