Material Description
Technical Data Sheet

Material Description

  • Material Properties:High mobility Chemical resistance High rigidity
  • Application Areas:Electrical applications electrical equipment
  • Color:--
  • Grade:Injection grade

Technical Data Sheet Compare

physical propertyTest ConditionTest MethodTest ResultUnit
Shrinkage rateFlow : 130°C, 1hrASTM D9551.6 到 1.8%
Shrinkage rateFlow : 3.20 mm内部方法1.1 到 1.3%
Shrinkage rateAcross Flow : 3.20 mm内部方法1.0 到 1.2%
Water absorption rate24 hr, 50% RHASTM D5700.50%
Water absorption rateEquilibrium, 50% RHASTM D5701.0%
Mechanical performanceTest ConditionTest MethodTest ResultUnit
Rockwell hardnessR-ScaleASTM D785116
tensile strengthYieldASTM D63859.0Mpa
tensile strengthBreakASTM D63855.0Mpa
elongationBreakASTM D63860%
Bending modulus100 mm SpanASTM D7902240Mpa
bending strengthYield, 100 mm SpanASTM D79095.0Mpa
Dart impact equipped with measuring instruments-30°C, Energy at PeakASTM D376339.0J
Dart impact equipped with measuring instruments23°C, Energy at PeakASTM D376350.0J
Thermal performanceTest ConditionTest MethodTest ResultUnit
Hot deformation temperature0.45 MPa, Unannealed, 6.40 mmASTM D648193°C
Hot deformation temperature1.8 MPa, Unannealed, 6.40 mmASTM D648143°C
vicat softening pointASTM D15254232°C
Linear coefficient of thermal expansionFlow : -40 to 95°CASTM E8319.0E-5cm/cm/°C
Linear coefficient of thermal expansionFlow : 60 to 138°CASTM E8311.3E-4cm/cm/°C
Linear coefficient of thermal expansionAcross Flow : -40 to 95°CASTM E8319.0E-5cm/cm/°C
Linear coefficient of thermal expansionAcross Flow : 60 to 138°CASTM E8311.3E-4cm/cm/°C
RTI ElecUL 74650.0°C
RTI ImpUL 74650.0°C
RTIUL 74650.0°C
Electrical performanceTest ConditionTest MethodTest ResultUnit
Arc resistanceASTM D495PLC 7
Compared to the Leakage Tracking Index (CTI)UL 746PLC 1
High arc combustion index (HAI)UL 746PLC 0
High Voltage Arc Traceability Rate (HVTR)UL 746PLC 4
Hot wire ignition (HWI)UL 746PLC 3
injectionTest ConditionTest MethodTest ResultUnit
drying temperature95 到 105°C
drying time3.0 到 4.0hr
Suggested maximum moisture content0.070%
Suggested injection volume30 到 50%
Temperature at the rear of the barrel265 到 305°C
Temperature in the middle of the barrel270 到 305°C
Temperature at the front of the material cylinder275 到 305°C
Spray nozzle temperature280 到 305°C
Processing (melt) temperature280 到 305°C
Mold temperature75 到 120°C
Back pressure0.300 到 1.40Mpa
Screw speed20 到 100rpm
Exhaust hole depth0.013 到 0.038mm
flammabilityTest ConditionTest MethodTest ResultUnit
UL flame retardant rating1.5 mmUL 94HB
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.