TPV Santoprene™ 8191-60B500 CELANESE USA

134
Unit Price:$3937 USD/MT
Packaging Specification:
25 KG/PKG
Supply Quantity:
10MT
Delivery Terms:
FOB
Port of Loading:
China Main Port
Accepted Payment Methods:
T/T
Shipping:
Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 2787 3515View
serv********View

For more detailed information including pricing, customization, and shipping, please contact supplier.

Material Description
Technical Data Sheet

Material Description

  • Material Properties:Chemical resistance Flame retardant
  • Application Areas:Profile building materials Kitchen utensils Parts under the hood of a Movable hinge Mirror frame Adhesive resin Soft handle Consumer product applicat Fatigue relief supplies Phone Bonding Application in the automo sporting goods Large and small household Home appliance components packing Electrical appliances
  • Color:--
  • Grade:Injection grade

Technical Data Sheet Compare

Mechanical performanceTest ConditionTest MethodTest ResultUnit
Shore hardnessShore A,15sec,23°CISO86853
ageingTest ConditionTest MethodTest ResultUnit
Change rate of tensile strength in air100°C,168hrASTMD573-28%
Change rate of tensile strength in air125°C,168hrASTMD573-61%
Change rate of tensile strength in air100°C,168hrISO188-28%
Change rate of tensile strength in air125°C,168hrISO188-61%
Change rate of hardness of hardness testerShoreA,23°C,168hr,inIRM903OilASTMD471-33
Change rate of hardness of hardness testerShoreA,23°C,168hr,inSodiumHydroxide,50%ASTMD4714.0
Change rate of hardness of hardness testerShoreA,23°C,168hr,inWaterASTMD4715.0
ChangeinShoreHardnessShoreA,23°C,168hr,inEthanol,95%ISO18172.0
ChangeinShoreHardnessShoreA,23°C,168hr,inHydrochloricAcid,10%ISO18174.0
ChangeinShoreHardnessShoreA,23°C,168hr,inIRM903OilISO1817-33
ChangeinShoreHardnessShoreA,23°C,168hr,inSodiumHydroxide,50%ISO18174.0
ChangeinShoreHardnessShoreA,23°C,168hr,inWaterISO18175.0
Change rate of ultimate elongation in air100°C,168hrASTMD573-14%
Change rate of ultimate elongation in air125°C,168hrASTMD573-70%
Changes in tensile stress during fracture in air100°C,168hrISO188-14%
Changes in tensile stress during fracture in air125°C,168hrISO188-70%
The rate of change in hardness of an air hardness testerShoreA,100°C,168hrASTMD573-4.0
The rate of change in hardness of an air hardness testerShore A,125°C,168hrASTMD5738.0
Change rate of Shore hardness in airShoreA,100°C,168hrISO188-4.0
Change rate of Shore hardness in airShore A,125°C,168hrISO1888.0
Change rate of tensile strength23°C,168hr,inEthanol,95%ASTMD471-17%
Change rate of tensile strength23°C,168hr,inHydrochloricAcid,10%ASTMD471-1.0%
Change rate of ultimate elongation23°C,168hr,inIRM903OilASTMD471-68%
Change rate of ultimate elongation23°C,168hr,inSodiumHydroxide,50%ASTMD471-7.0%
Change rate of ultimate elongation23°C,168hr,在水中ASTMD471-12%
Changes in tensile stress during fracture23°C,168hr,inEthanol,95%ISO1817-3.0%
Changes in tensile stress during fracture23°C,168hr,inHydrochloricAcid,10%ISO1817-9.0%
Changes in tensile stress during fracture23°C,168hr,inIRM903OilISO1817-68%
Changes in tensile stress during fracture23°C,168hr,inSodiumHydroxide,50%ISO1817-7.0%
Changes in tensile stress during fracture23°C,168hr,在水中ISO1817-12%
Change rate of hardness of hardness testerShoreA,23°C,168hr,inEthanol,95%ASTMD4712.0
Change rate of hardness of hardness testerShoreA,23°C,168hr,inHydrochloricAcid,10%ASTMD4714.0
Change rate of tensile strength23°C,168hr,inIRM903OilASTMD471-85%
Change rate of tensile strength23°C,168hr,inSodiumHydroxide,50%ASTMD4711.0%
Change rate of tensile strength23°C,168hr,在水中ASTMD4712.0%
Change rate of tensile strength23°C,168hr,inEthanol,95%ISO1817-17%
Change rate of tensile strength23°C,168hr,inHydrochloricAcid,10%ISO1817-1.0%
Change rate of tensile strength23°C,168hr,inIRM903OilISO1817-85%
Change rate of tensile strength23°C,168hr,inSodiumHydroxide,50%ISO18171.0%
Change rate of tensile strength23°C,168hr,在水中ISO18172.0%
Change rate of ultimate elongation23°C,168hr,inEthanol,95%ASTMD471-3.0%
Change rate of ultimate elongation23°C,168hr,inHydrochloricAcid,10%ASTMD471-9.0%
elastomerTest ConditionTest MethodTest ResultUnit
Elongation rate - lateral flow rateBreak,23°CASTMD412600%
Elongation rate - lateral flow rateBreak,23°CISO37600%
CompressionSet125°C,70hrASTMD395B55%
CompressionSet125°C,70hrISO81555%
flammabilityTest ConditionTest MethodTest ResultUnit
UL flame retardant rating1.1mmUL94HB
UL flame retardant rating3.0mmUL94HB
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.