PBT LNP™ LUBRICOMP™  WL004 WHNAT SABIC INNOVATIVE US

146
Unit Price:$4272 USD/MT
Packaging Specification:
25 KG/PKG
Supply Quantity:
97.5MT
Delivery Terms:
FOB
Port of Loading:
China Main Port
Accepted Payment Methods:
T/T
Shipping:
Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 2787 3515View
serv********View

For more detailed information including pricing, customization, and shipping, please contact supplier.

Material Description
Technical Data Sheet

Material Description

  • Material Properties:wear resistant
  • Application Areas:Electronic and ElectricalElectrical appliances
  • Color:--
  • Grade:Injection grade

Technical Data Sheet Compare

PhysicalTest ConditionTest MethodTest Result
Modeling ShrinkageMD:24小时ASTMD9552.1to2.4 %
Modeling ShrinkageTD:24hrASTMD9552.1to2.4 %
Modeling ShrinkageTD:24小时ISO294-42.1to2.3 %
Modeling ShrinkageMD:24小时ISO294-42.4to2.5 %
Moisture Absorption24hr,50%RHASTMD5700.051 %
Moisture Absorption平衡,23°C,50%RHISO620.080 %
Thermal PropertiesTest ConditionTest MethodTest Result
Linear thermal expansion coefficientMD:-40到40°CISO11359-29E-05 cm/cm/°C
Linear thermal expansion coefficientTD:-40到40°CASTME8319.6E-05 cm/cm/°C
Linear thermal expansion coefficientTD:-40到40°CISO11359-29.6E-05 cm/cm/°C
Heat Deflection Temperature1.8MPa,未退火,3.20mmASTMD64855.0 °C
Heat Deflection Temperature1.8MPa,未退火,64.0mm跨距ISO75-2/Af61.0 °C
Linear thermal expansion coefficientMD:-40到40°CASTME8319E-05 cm/cm/°C
Mechanical PropertiesTest ConditionTest MethodTest Result
Tensile Strength断裂ASTMD63849.0 Mpa
Tensile Stress断裂ISO527-245.0 Mpa
Tensile Elongation断裂ASTMD6389.8 %
Tensile Strain断裂ISO527-28.4 %
Flexural ModulusASTMD7902410 Mpa
Flexural ModulusISO1782390 Mpa
Flexural StrengthASTMD79078.7 Mpa
Flexural StressISO17877.1 Mpa
Coefficient of FrictionDynamicASTMD3702Modified0.33
Coefficient of FrictionStaticASTMD3702Modified0.24
Tensile ModulusASTMD6382410 Mpa
Tensile ModulusISO527-2/12450 Mpa
Specific Wear RateASTMD3702Modified58.0 10^-10in^5-min/ft-lb-hr
Impact PropertiesTest ConditionTest MethodTest Result
Notched Izod Impact Strength23°CISO180/1A3.6 kJ/m²
UnnotchedIzodImpactStrength323°CISO180/1U30 kJ/m²
Instrumented Dart Impact23°C,EnergyatPeakLoadASTMD37630.960 J
Multi-Axial Instrumented Impact EnergyISO6603-20.500 J
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.