PPS FORTRON® 1140L6 SF3001 CELANESE USA

174
Unit Price:$7709 USD/MT
Packaging Specification:
25 KG/PKG
Supply Quantity:
23.5MT
Delivery Terms:
FOB
Port of Loading:
China Main Port
Accepted Payment Methods:
T/T
Shipping:
Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 2787 3515View
serv********View

For more detailed information including pricing, customization, and shipping, please contact supplier.

Material Description
Technical Data Sheet

Material Description

  • Material Properties:Flame retardant Glass fiber reinforced High temperature resistan
  • Application Areas:fibre Bottle cap
  • Color:--
  • Grade:Injection grade

Technical Data Sheet Compare

物理性能Test ConditionTest MethodTest ResultUnit
收缩率MDASTMD9550.20to0.30%
收缩率TDASTMD9550.50to0.70%
收缩率TDISO294-40.40to0.60%
收缩率MDISO294-40.20to0.60%
收缩率ISO 25770.2-0.6%
吸水率ISO 620.02%
吸水率饱和,23°CISO620.020%
SpecificHeatCapacityofMelt内部方法1500J/kg/°C
特定体积ASTMD7920.625cm³/g
SpiralFlow内部方法21.5
熔体质量流动速率ASTMD123819g/10min
密度ISO11831.65g/cm³
密度ISO 11831.65g/cm³
密度ASTMD7921.60g/cm³
机械性能Test ConditionTest MethodTest ResultUnit
悬臂梁无缺口冲击强度23°CISO180/1U34kJ/m²
简支梁缺口冲击强度-30°CISO179/1eA10kJ/m²
简支梁缺口冲击强度23°CISO179/1eA10kJ/m²
悬壁梁缺口冲击强度-30°CISO180/1A10kJ/m²
悬壁梁缺口冲击强度23°CISO180/1A10kJ/m²
悬臂梁缺口冲击强度23℃ISO 180/1A10kJ/m²
简支梁无缺口冲击强度-30°CISO179/1eU53kJ/m²
简支梁无缺口冲击强度23°CISO179/1eU53kJ/m²
拉伸模量ISO 527-114700Mpa
拉伸模量ISO527-2/1A/114700Mpa
拉伸强度ISO 527-1195Mpa
拉伸强度断裂,23°CASTMD638200Mpa
拉伸强度断裂ISO527-2/1A/5195Mpa
伸长率断裂,23°CASTMD6382.0%
伸长率断裂ISO527-2/1A/51.9%
伸长率断裂ISO 527-11.9%
洛氏硬度ISO 2039-2100M-scale
洛氏硬度M级ASTMD785100
洛氏硬度M级ISO2039-2100
弯曲模量ISO 17814500Mpa
弯曲模量23°CISO17814500Mpa
弯曲强度ISO178285Mpa
弯曲强度ISO 178285Mpa
热性能Test ConditionTest MethodTest ResultUnit
熔融温度ISO11357-3280°C
阻燃等级UL94V-0
线性热膨胀系数MDISO11359-22.6E-05cm/cm/°C
线性热膨胀系数TDISO11359-24.2E-05cm/cm/°C
玻璃转化温度ISO11357-290.0°C
热变形温度1.80MpaISO 75-1270°C
热变形温度0.45MPa,退火ASTMD648280°C
热变形温度1.8MPa,未退火ASTMD648265°C
热变形温度1.8MPa,未退火ISO75-2/A270°C
热变形温度8.0MPa,未退火ISO75-2/C215°C
电气性能Test ConditionTest MethodTest ResultUnit
耗散因数1kHzASTMD1501E-03
耗散因数1MHzASTMD1501E-03
耗散因数1MHzIEC602502E-03
介电强度IEC60243-128KV/mm
相对电容率1MHzIEC602504.10
漏电起痕指数IEC60112125V
介电强度ASTMD14915KV/mm
表面电阻率IEC60093>1.0E+15ohms
介电常数1kHzASTMD1503.50
介电常数1MHzASTMD1503.50
耐电弧性ASTMD495134sec
体积电阻率ASTMD2571E+16ohms·cm
体积电阻率IEC60093>1.0E+15ohms·cm
可燃性Test ConditionTest MethodTest ResultUnit
UL阻燃等级0.38mmUL94V-0
UL阻燃等级1.5mmUL94V-0
补充信息Test ConditionTest MethodTest ResultUnit
CSARating8.40E-7mmCSAF-1A00
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.