PC/ABS LNP™ THERMOCOMP™ NX07344 BK1E257 SABIC INNOVATIVE US
136
Unit Price:$5400 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 23MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:High mobility|Flame retardant
- Application Areas:Casters|Electrical applications
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical | Test Condition | Test Method | Test Result |
---|---|---|---|
Modeling Shrinkage | MD | 内部方法 | 0.38 % |
TD | 内部方法 | 0.46 % | |
24hr,50%RH | ASTMD570 | 0.080 % | |
Equilibrium,23°C,50%RH | ISO62 | 0.040 % |
Thermal Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Flow:23 to 60°C | ISO11359-2 | 2.9E-05 cm/cm/°C | |
Flow:-40 to 40°C | ASTME831 | 5.8E-05 cm/cm/°C | |
Flow:23 to 60°C | ISO11359-2 | 7.4E-05 cm/cm/°C | |
1.8MPa, Unannealed,3.20mm | ASTMD648 | 94.0 °C | |
1.8MPa, Unannealed,6.40mm | ASTMD648 | 96.0 °C | |
1.8MPa, Unannealed,64.0mm Span | ISO75-2/Af | 96.0 °C | |
Flow:-40 to 40°C | ASTME831 | 3.1E-05 cm/cm/°C |
Flammability | Test Condition | Test Method | Test Result |
---|---|---|---|
Flame Rating | 1.50mm | UL94 | V-0 |
Electrical Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Surface Resistivity | ASTMD257 | 1.0E+3到1.0E+6 ohms | |
Volume Resistivity | ASTMD257 | 1.0E+4到1.0E+6 ohms·cm | |
StaticDecay17 | FTMS101B | 10 msec | |
EMI Attenuation | 1.50mm | 内部方法 | 47到53 dB |
3.00mm | 内部方法 | 60到70 dB |
Mechanical Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Break,50.0mm Span | ASTMD790 | 90.0 Mpa | |
Flexural Strain (Break) | ISO178 | 2.8 % | |
--1 | ASTMD638 | 6000 Mpa | |
Break | ASTMD638 | 60.0 Mpa | |
fracture | ISO527-2/5 | 62.0 Mpa | |
Break | ASTMD638 | 1.8 % | |
fracture | ISO527-2/5 | 1.8 % | |
Flexural Modulus | 50.0mm跨距 | ASTMD790 | 5300 Mpa |
--5 | ISO178 | 105 Mpa | |
Yield,50.0mm Span | ASTMD790 | 90.0 Mpa |
Impact Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Charpy Notched Impact Strength | 23°C | ISO179/1eA | 7.6 kJ/m² |
-30°C | ASTMD256 | 44 J/m | |
23°C | ASTMD256 | 60 J/m | |
-30°C10 | ISO180/1A | 5.3 kJ/m² | |
23°C11 | ISO180/1A | 6.0 kJ/m² | |
-30°C | ASTMD4812 | 330 J/m | |
23°C | ASTMD4812 | 350 J/m | |
-30°C12 | ISO180/1U | 21 kJ/m² | |
23°C13 | ISO180/1U | 21 kJ/m² | |
23°C,TotalEnergy | ASTMD3763 | 11.5 J |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.