PC LNP™ THERMOCOMP™ D151-7A1D317 SABIC INNOVATIVE US
150
Unit Price:$3992 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 97MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Glass fiber reinforced|Non chloro non bromine fl
- Application Areas:Electronic and Electrical|Plastic bag
- Color:--
- Grade:--
Technical Data Sheet
Physical | Test Condition | Test Method | Test Result |
---|---|---|---|
Melt Mass-Flow Rate | 300°C/1.2kg | ASTMD1238 | 14 g/10min |
300°C/2.16kg | ASTMD1238 | 29 g/10min | |
Melt Volume flow Rate | 300°C/1.2kg | ISO1133 | 13.0 cm3/10min |
300°C/2.16kg | ISO1133 | 27.0 cm3/10min | |
Modeling Shrinkage | MD:24小时 | ASTMD955 | 0.30到0.50 % |
TD:24小时 | ASTMD955 | 0.30到0.50 % | |
Moisture Absorption | 饱和,23°C | ISO62 | 0.080 % |
平衡,23°C,50%RH | ISO62 | 0.040 % |
Thermal Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Linear thermal expansion coefficient | TD:23到80°C | ISO11359-2 | 7.7E-05 cm/cm/°C |
Heat Deflection Temperature | 0.45MPa,未退火,3.20mm | ASTMD648 | 121 °C |
1.8MPa,未退火,3.20mm | ASTMD648 | 117 °C | |
Linear thermal expansion coefficient | MD:23到80°C | ISO11359-2 | 3.4E-05 cm/cm/°C |
Flammability | Test Condition | Test Method | Test Result |
---|---|---|---|
Flame Rating | 0.300mm | UL94 | V-2 |
0.400mm | UL94 | V-1 | |
0.600mm | UL94 | V-0 |
Electrical Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Dielectric Constant | 1.10GHz | 内部方法 | 3.07 |
1.90GHz | 内部方法 | 3.06 | |
5.00GHz | 内部方法 | 3.06 | |
10.0GHz | 内部方法 | 3.05 | |
Dissipation Factor? | 1.10GHz | 内部方法 | 6.7E-03 |
1.90GHz | 内部方法 | 6.5E-03 | |
5.00GHz | 内部方法 | 6.9E-03 | |
10.0GHz | 内部方法 | 6.9E-03 |
Mechanical Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
--6 | ISO178 | 133 Mpa | |
Break,50.0mm Span | ASTMD790 | 131 Mpa | |
--1 | ASTMD638 | 4400 Mpa | |
Break | ASTMD638 | 83.0 Mpa | |
fracture | ISO527-2/5 | 82.0 Mpa | |
Break | ASTMD638 | 3.6 % | |
fracture | ISO527-2/5 | 3.6 % | |
50.0mm Span | ASTMD790 | 4070 Mpa | |
--5 | ISO178 | 4010 Mpa |
Impact Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Charpy Notched Impact Strength | 23°C | ISO179/1eA | 13 kJ/m² |
Charpy Unnotched Impact Strength | 23°C | ISO179/1eU | 50 kJ/m² |
Unnotched Izod Impact Strength | 23°C | ASTMD4812 | 710 J/m |
Instrumented Dart Impact | 23°C,EnergyatPeakLoad | ASTMD3763 | 22.0 J |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.