PC LEXAN™ 500-131 SABIC INNOVATIVE US
106
Unit Price:$2692 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Flame retardant|Glass fiber reinforced|Filler: Glass fiber reinf|10% filler by weight
- Application Areas:Automotive Applications|household electrical appl|fibre
- Color:--
- Grade:Enhanced level
Technical Data Sheet
Physical | Test Condition | Test Method | Test Result |
---|---|---|---|
Specific Volume | ASTMD792 | 0.802 cm³/g | |
Density / Specific Gravity | ASTMD792 | 1.27 g/cm³ | |
ASTMD792 | 1.25 g/cm³ | ||
Melt Mass-Flow Rate | 300°C/1.2kg | ASTMD1238 | 7.5 g/10min |
Modeling Shrinkage | MD:3.20mm | 内部方法 | 0.20to0.40 % |
Moisture Absorption | 24hr | ASTMD570 | 0.12 % |
平衡,23°C | ASTMD570 | 0.31 % | |
Outdoor Suitability | UL746C | f2 |
Thermal Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Heat Deflection Temperature | 0.45MPa,未退火,6.40mm | ASTMD648 | 146 °C |
1.8MPa,未退火,6.40mm | ASTMD648 | 142 °C | |
Vicat Softening Temperature | ASTMD15255 | 154 °C | |
Linear thermal expansion coefficient | MD:-40到95°C | ASTME831 | 3.2E-05 cm/cm/°C |
Specific Heat | ASTMC351 | 1210 J/kg/°C | |
Thermal Conductivity | ASTMC177 | 0.20 W/m/K | |
RTIElec | UL746 | 130 °C | |
Evolution Calendar intelligent importer | UL746 | 130 °C | |
RTIStr | UL746 | 130 °C |
Flammability | Test Condition | Test Method | Test Result |
---|---|---|---|
Radiant Panel Listing | UL | YES | |
Flame Rating | 1.5mm | UL94 | V-0 |
3.0mm | UL94 | 5VA | |
Oxygen Index | ASTMD2863 | 36 % |
Electrical Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
High Voltage Arc Tracking Rate | HVTR | UL746 | PLC 4 |
High Amp Arc Ignition | HAI | UL746 | PLC 4 |
Hot-wire Ignition | HWI | UL746 | PLC 1 |
Dielectric Constant | 1MHz | ASTMD150 | 3.05 |
Dissipation Factor? | 50Hz | ASTMD150 | 8E-04 |
60Hz | ASTMD150 | 8E-04 | |
Arc Resistance | ASTMD495 | PLC7 | |
Dissipation Factor? | 1MHz | ASTMD150 | 7.5E-03 |
Comparative Tracking Index | CTI | UL746 | PLC 3 |
Volume Resistivity | ASTMD257 | >1.0E+17 ohms·cm | |
Dielectric Constant | 50Hz | ASTMD150 | 3.10 |
Dielectric Strength | 3.20mm,inAir | ASTMD149 | 18 KV/mm |
Dielectric Constant | 60Hz | ASTMD150 | 3.10 |
Mechanical Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile Elongation | 断裂 | ASTMD638 | 15 % |
屈服 | ASTMD638 | 8.0 % | |
Flexural Modulus | 50.0mm跨距 | ASTMD790 | 3450 Mpa |
Flexural Strength | 屈服,50.0mm跨距 | ASTMD790 | 103 Mpa |
Taber Abrasion Resistance | 1000Cycles,1000g,CS-17转轮 | ASTMD1044 | 11.0 mg |
Tensile Strength | 屈服 | ASTMD638 | 66.2 Mpa |
断裂 | ASTMD638 | 55.2 Mpa |
Hardness | Test Condition | Test Method | Test Result |
---|---|---|---|
Rockwell Hardness | M计秤 | ASTMD785 | 85 |
R计秤 | ASTMD785 | 124 |
Impact Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Notched Izod Impact Strength | 23°C | ASTMD256 | 110 J/m |
23°C | ASTMD4812 | 2100 J/m | |
Gardner Impact | 23°C | ASTMD3029 | 102 J |
Tensile Impact Strength | ASTMD1822 | 158 kJ/m² |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.
Contact Us
Get App
Top