PC PANLITE® L-1225Y BK TEIJIN JAPAN
241
Unit Price:$3144 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 18.8MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Low viscosity|transparent|High mobility
- Application Areas:Electrical appliances|Casters|Household appliances|Mechanical components|Medical supplies|Labor protection equipmen|container|Electronic field|Electrical field|Application in the automo|Car headlights
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical | Test Condition | Test Method | Test Result |
---|---|---|---|
Density / Specific Gravity | ISO1183 | 1.20 g/cm³ | |
Melt Volume flow Rate | 300°C/1.2kg | ISO1133 | 25.0 cm3/10min |
Modeling Shrinkage | TD:4.00mm | 内部方法 | 0.50to0.70 % |
MD:4.00mm | 内部方法 | 0.50to0.70 % | |
Moisture Absorption | 23°C,24hr | ISO62 | 0.20 % |
Thermal Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
RTIElec | 1.5mm | UL746 | 125 °C |
Evolution Calendar intelligent importer | 1.5mm | UL746 | 115 °C |
RTIStr | 1.5mm | UL746 | 125 °C |
Heat Deflection Temperature | 0.45MPa,未退火 | ISO75-2/B | 136 °C |
1.8MPa,未退火 | ISO75-2/A | 123 °C | |
Vicat Softening Temperature | ISO306/B50 | 142 °C | |
Linear thermal expansion coefficient | MD | ISO11359-2 | 7E-05 cm/cm/°C |
TD | ISO11359-2 | 7E-05 cm/cm/°C |
Optical | Test Condition | Test Method | Test Result |
---|---|---|---|
Index of Refraction | ASTMD542 | 1.585 | |
Transmittance | 3000µm | ASTMD1003 | 88.0 % |
Flammability | Test Condition | Test Method | Test Result |
---|---|---|---|
Flame Rating | 2.1mm | UL94 | HB |
0.40mm | UL94 | V-2 | |
Glow Wire Flammability Index | 1.5mm | IEC60695-2-12 | 825 °C |
3.2mm | IEC60695-2-12 | 875 °C | |
Glow Wire Ignition Temperature | 1.5mm | IEC60695-2-13 | 850 °C |
3.2mm | IEC60695-2-13 | 875 °C |
Electrical Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Surface Resistivity | IEC60093 | >1.0E+15 ohms | |
Volume Resistivity | IEC60093 | >1.0E+15 ohms·cm | |
Dielectric Strength | IEC60243-1 | 30 KV/mm | |
Relative Permittivity | 100Hz | IEC60250 | 3.10 |
1MHz | IEC60250 | 3.00 | |
Dissipation Factor? | 100Hz | IEC60250 | 1E-03 |
1MHz | IEC60250 | 9E-03 | |
Comparative Tracking Index | IEC60112 | 250 V |
Mechanical Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile Modulus | ISO527-2/1 | 2400 Mpa | |
Tensile Stress | 屈服 | ISO527-2/50 | 62.0 Mpa |
Tensile Strain | 屈服 | ISO527-2/50 | 6.0 % |
Nominal Tensile Strain at Break | ISO527-2/50 | >50 % | |
Flexural Modulus | ISO178 | 2400 Mpa | |
Flexural Stress | ISO178 | 95.0 Mpa |
Impact Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Charpy Notched Impact Strength | ISO179 | 53 kJ/m² | |
Charpy Unnotched Impact Strength | ISO179 | NoBreak |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.