PC LEXAN™ 143R SABIC INNOVATIVE US
106
Unit Price:$3248 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Material Certification
Technical Data Sheet
Material Description
- Material Properties:UV resistance|Weather resistance|Low viscosity
- Application Areas:film|Electric wire|Cable
- Color:--
- Grade:Injection grade
Material Certification

Technical Data Sheet
Physical | Test Condition | Test Method | Test Result |
---|---|---|---|
Moisture Absorption | 平衡,100°C | ASTMD570 | 0.58 % |
Outdoor Suitability | UL746C | f1 | |
Moisture Absorption | 平衡,23°C | ASTMD570 | 0.35 % |
24hr | ASTMD570 | 0.15 % | |
Modeling Shrinkage | MD:3.20mm | 内部方法 | 0.50到0.70 % |
Melt Mass-Flow Rate | 300°C/1.2kg | ASTMD1238 | 11 g/10min |
Specific Volume | ASTMD792 | 0.835 cm³/g | |
Density / Specific Gravity | -- | ASTMD792 | 1.19 g/cm³ |
-- | ASTMD792 | 1.20 g/cm³ |
Thermal Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
RTI | UL746 | 130 °C | |
RTIElec | UL746 | 130 °C | |
Evolution Calendar intelligent importer | UL746 | 130 °C | |
Thermal Conductivity | ASTMC177 | 0.19 W/m/K | |
Linear thermal expansion coefficient | MD:-40到95°C | ASTME831 | 6.8E-05 cm/cm/°C |
Specific Heat | ASTMC351 | 1260 J/kg/°C | |
Vicat Softening Temperature | ASTMD15256 | 154 °C | |
Heat Deflection Temperature | 1.8MPa,未退火,6.40mm | ASTMD648 | 132 °C |
0.45MPa,未退火,6.40mm | ASTMD648 | 138 °C |
Optical | Test Condition | Test Method | Test Result |
---|---|---|---|
Haze | 2540µm | ASTMD1003 | 1.0 % |
Transmittance | 2540µm | ASTMD1003 | 88.0 % |
Index of Refraction | ASTMD542 | 1.586 |
Flammability | Test Condition | Test Method | Test Result |
---|---|---|---|
Flame Rating | 0.762mm | UL94 | HB |
Oxygen Index | ASTMD2863 | 25 % |
Electrical Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Comparative Tracking Index | CTI | UL746 | PLC 2 |
High Amp Arc Ignition | HAI | UL746 | PLC 1 |
Dissipation Factor? | 1MHz | ASTMD150 | 0.010 |
60Hz | ASTMD150 | 9E-04 | |
50Hz | ASTMD150 | 9E-04 | |
Dielectric Constant | 1MHz | ASTMD150 | 2.96 |
60Hz | ASTMD150 | 3.17 | |
50Hz | ASTMD150 | 3.17 | |
Dielectric Strength | 3.20mm,inAir | ASTMD149 | 15 KV/mm |
Volume Resistivity | ASTMD257 | >1.0E+17 ohms·cm | |
High Voltage Arc Tracking Rate | HVTR | UL746 | PLC 2 |
Hot-wire Ignition | HWI | UL746 | PLC 4 |
Mechanical Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Flexural Strength | 屈服,50.0mm跨距 | ASTMD790 | 93.1 Mpa |
Flexural Modulus | 50.0mm跨距 | ASTMD790 | 2340 Mpa |
Tensile Elongation | 断裂 | ASTMD638 | 110 % |
屈服 | ASTMD638 | 7.0 % | |
Tensile Strength | 断裂 | ASTMD638 | 65.5 Mpa |
屈服 | ASTMD638 | 62.1 Mpa | |
Taber Abrasion Resistance | 1000Cycles,1000g,CS-17转轮 | ASTMD1044 | 10.0 mg |
Hardness | Test Condition | Test Method | Test Result |
---|---|---|---|
Rockwell Hardness | R级 | ASTMD785 | 118 |
M级 | ASTMD785 | 70 |
Impact Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile Impact Strength | ASTMD1822 | 546 kJ/m² | |
Gardner Impact | 23°C | ASTMD3029 | 169 J |
Notched Izod Impact Strength | 23°C | ASTMD256 | 800 J/m |
Unnotched Izod Impact Strength | 23°C | ASTMD4812 | 3200 J/m |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.