LLDPE DOWLEX™ 2036P DOW SPAIN
140
Unit Price:$1569 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 28MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:--
- Application Areas:--
- Color:--
- Grade:Blow molding grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
density | ASTM D-792 | 0.935 | g/m3 | |
Melt flow rate | ASTM D-1238 | 2.5 | g/10min | |
film thickness | 25.4 | um | ||
Melt mass flow rate | 190°C/2.16kg | ASTMD1238 | 2.5 | g/10min |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile yield strength (MD) | 25.4um | ASTM D-882 | 17.6 | Mpa |
25.4um | ASTM D-882 | 16.9 | Mpa | |
Tensile fracture strength (TD) | 25.4um | ASTM D-882 | 39.9 | Mpa |
Tensile strength at break (MD) | 25.4um | ASTM D-882 | 59.2 | Mpa |
Tensile elongation at break (MD) | 25.4um | ASTM D-882 | 620 | % |
Tensile elongation at break (TD) | 25.4um | ASTM D-882 | 750 | % |
Falling hammer impact | 25.4um | ASTM D-1709A | 57 | g |
Elmendorf Tear Strength (MD) | 25.4um | ASTM D-1922 | 83 | g |
Elmendorf Tear Strength (TD) | 25.4um | ASTM D-1922 | 290 | g |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
vicat softening point | ASTM D-1525 | 119 | °C | |
Melting temperature | Internal Method | 125 | °C | |
vicat softening point | ASTMD1525 | 119 | °C | |
Melting temperature | 内部方法 | 125 | °C |
film | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Film thickness - tested | 25 | µm | ||
Membrane puncture resistance | 25µm | 内部方法 | 10.3 | J/cm³ |
Membrane strength | MD:25µm | ASTMD882 | 324 | J/cm³ |
TD:25µm | ASTMD882 | 308 | J/cm³ | |
Tensile strength | MD:Yield,25μm | ASTMD882 | 16.9 | Mpa |
TD:Yield,25μm | ASTMD882 | 17.6 | Mpa | |
MD:Break,25μm | ASTMD882 | 59.2 | Mpa | |
TD:Break,25μm | ASTMD882 | 39.9 | Mpa | |
elongation | MD:Break,25μm | ASTMD882 | 620 | % |
TD:Break,25μm | ASTMD882 | 750 | % | |
Falling hammer impact | 25µm | ASTMD1709A | 57 | g |
Elmondov tear strength | MD:25µm | ASTMD1922 | 83 | g |
TD:25µm | ASTMD1922 | 290 | g |
Other performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Film Piercing Resistance Movement | 25.4um | Internal Method | 10.3 | J/cm³ |
Film Resilience (MD) | 25.4um | ASTM D-882 | 324 | J/cm³ |
Film Resilience (TD) | 25.4um | ASTM D-882 | 308 | J/cm4 |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
gloss | 45°,25.4µm | ASTMD2457 | 90 | |
Haze | 25.4µm | ASTMD1003 | 2.6 | % |
gloss | 45°,25.4um | ASTM D-2457 | 90 | |
Haze | 25.4um | ASTM D-1003 | 2.6 | % |
Processing conditions | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Melt Temperature | 274 | °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.