PA66 Zytel® 158 NC010Z DUPONT USA
118
Unit Price:$3632 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 30MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:High temperature resistan Glass fiber reinforced
- Application Areas:electrical equipment Fitness equipment
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
MediumDensity | 0.900 | g/cm³ | ||
SpecificHeatCapacity of Melt | 2800 | J/kg/°C | ||
ThermalConductivityofMelt | 0.19 | W/m/K | ||
Shrinkage rate | MD:3.20mm | 1.1 | % | |
TD | ISO294-4 | 1.4 | % | |
MD | ISO294-4 | 1.3 | % | |
Water absorption rate | Saturation,23°C,2.00mm | ISO62 | 3.0 | % |
Equilibrium,23°C,2.00mm,50%RH | ISO62 | 1.3 | % | |
Stickiness number | ISO307 | 120 | cm³/g |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile modulus | ISO527-2 | 2400 | Mpa | |
tensile strength | Yield | ISO527-2 | 62.0 | Mpa |
elongation | Yield | ISO527-2 | 4.5 | % |
Nominal tensile fracture strain | ISO527-2 | 35 | % | |
Bending modulus | ISO178 | 2050 | Mpa | |
Impact strength of simply supported beam without notch | -30°C | ISO179/1eU | NoBreak | |
23°C | ISO179/1eU | NoBreak |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hot deformation temperature | 0.45MPa,Unannealed | ISO75-2/B | 135 | °C |
1.8MPa,Unannealed | ISO75-2/A | 62.0 | °C | |
Glass transition temperature | ISO11357-2 | 60.0 | °C | |
Melting temperature | ISO11357-3 | 218 | °C | |
Linear coefficient of thermal expansion | MD:-- | ISO11359-2 | 1.2E-04 | cm/cm/°C |
MD:-40to23°C | ISO11359-2 | 9E-05 | cm/cm/°C | |
MD:55to160°C | ISO11359-2 | 1.7E-04 | cm/cm/°C | |
TD:-- | ISO11359-2 | 1.2E-04 | cm/cm/°C | |
TD:-40to23°C | ISO11359-2 | 9E-05 | cm/cm/°C | |
TD:55to160°C | ISO11359-2 | 1.8E-04 | cm/cm/°C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Surface resistivity | IEC60093 | -- | ohms | |
Volume resistivity | IEC60093 | >1.0E+15 | ohms·cm | |
Dielectric strength | IEC60243-1 | 36 | KV/mm | |
Relative permittivity | 100Hz | IEC60250 | 3.60 | |
1MHz | IEC60250 | 3.20 | ||
Dissipation factor | 100Hz | IEC60250 | 0.014 | |
1MHz | IEC60250 | 0.016 |
flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Burning rate | 1.00mm | ISO3795 | <100 | mm/min |
UL flame retardant rating | 0.9mm | UL94 | HB | |
1.5mm | UL94 | HB | ||
0.9mm | IEC60695-11-10,-20 | HB | ||
1.5mm | IEC60695-11-10,-20 | HB | ||
Extreme Oxygen Index | ISO4589-2 | 25 | % | |
FMVSS flammability | FMVSS302 | B |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.