PA66 UBE 2020GC4 UBE JAPAN

162
Unit Price:$2850 USD/MT
Packaging Specification:
25 KG/PKG
Supply Quantity:
28.8MT
Delivery Terms:
FOB
Port of Loading:
China Main Port
Accepted Payment Methods:
T/T
Shipping:
Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 2787 3515View
serv********View

For more detailed information including pricing, customization, and shipping, please contact supplier.

Material Description
Technical Data Sheet

Material Description

  • Material Properties:Glass fiber reinforced
  • Application Areas:--
  • Color:--
  • Grade:Injection grade

Technical Data Sheet Compare

physical propertyTest ConditionTest MethodTest ResultUnit
densityASTM D792/ISO 11831.28
Water absorption rate 23 ℃/24hASTM D570/ISO 621%
Water absorption rateASTM D-5701.0%
Water absorption rateASTM D-5706.6%
Shrinkage rateUBEmethod0.6%
Shrinkage rateUBEmethod1.4%
Mechanical performanceTest ConditionTest MethodTest ResultUnit
Flexural elasticity23°ASTM D-79065000Kgf/cm
Hardness (Rockwell, Brinell)23°ASTM D-78595
Impact strength of cantilever beam gapASTM D256/ISO 1797kg·cm/cm(J/M)ft·lb/in
Rockwell hardnessASTM D785120
Bending modulusASTM D790/ISO 17865000kg·cm/cm(J/M)ft·lb/in
bending strengthASTM D790/ISO 1782200kg·cm/cm(J/M)ft·lb/in
Tensile strength under yield23°ASTM D-638950Kgf/cm
Flexural elasticity23°ASTM D-79040000Kgf/cm
Tensile strength under yield23°ASTM D-6381550Kgf/cm
Hardness (Rockwell, Brinell)23°ASTM D-785120
Hardness (Rockwell, Brinell)23°ASTM D-785113
Impact resistance strength23°ASTM D-25610Kgf.cm/cm
bending strength23°ASTM D-7901400Kgf/cm
bending strength23°ASTM D-7902200Kgf/cm
Impact resistance strength23°ASTM D-2567.0Kgf.cm/cm
Elongation under fracture23°ASTM D-6385%
Thermal performanceTest ConditionTest MethodTest ResultUnit
Hot deformation temperatureASTM D648/ISO 75252℃(℉)
melting point255-265℃(℉)
Linear coefficient of thermal expansionASTM D696/ISO 113593.5mm/mm.℃
melting pointDSC215-225°C
Hot deformation temperature8.6kgf/cmASTM D-648252°C
Linear coefficient of thermal expansionASTM D-6963.5X的10
Combustion rateUL 94HB
Electrical performanceTest ConditionTest MethodTest ResultUnit
Volume resistivityASTM D257/IEC 6009310^15Ω.cm
Insulation EnduranceASTM D-1492KV/mm
Volume resistivityASTM D-25710Ω.cm
Dielectric loss10ASTM D-1500.01
Dielectric constant10ASTM D-1504.0
Dielectric constant10ASTM D-1503.6
IEC circuitUL 746600V
Dielectric constant60HZASTM D-1504.1
Dielectric loss60HZASTM D-1500.01
Arc resistance strengthASTM D-495151S
Dielectric loss10ASTM D-1500.02
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.