PA6 Zytel® 73G30T BK261 DUPONT USA
172
Unit Price:$2967 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 102MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Thermal stability Filler: Glass fiber reinf 30% filler by weight
- Application Areas:Automotive Applications Electronic and electrical
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
density | ISO1183 | 1.35 | g/cm³ | |
Shrinkage rate | TD | ISO294-4 | 1.0 | % |
MD | ISO294-4 | 0.20 | % | |
Water absorption rate | Saturation,23°C,2.00mm | ISO62 | 6.2 | % |
Equilibrium,23°C,2.00mm,50%RH | ISO62 | 1.8 | % | |
MediumDensity | 1.31 | g/cm³ | ||
Top out temperature | 210 | °C | ||
SpecificHeatCapacity of Melt | 2200 | J/kg/°C | ||
ThermalConductivityofMelt | 0.23 | W/m/K |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile modulus | ISO527-2 | 9500 | Mpa | |
Tensile stress | Break | ISO527-2 | 160 | Mpa |
Tensile strain | Break | ISO527-2 | 3.3 | % |
Impact strength of simply supported beam gap | -30°C | ISO179/1eA | 10 | kJ/m² |
23°C | ISO179/1eA | 14 | kJ/m² |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hot deformation temperature | 0.45MPa,Unannealed | ISO75-2/B | 210 | °C |
1.8MPa,Unannealed | ISO75-2/A | 206 | °C | |
vicat softening point | ISO306/B50 | 210 | °C | |
Melting temperature | ISO11357-3 | 220 | °C | |
Linear coefficient of thermal expansion | MD2 | ISO11359-2 | 3E-05 | cm/cm/°C |
TD2 | ISO11359-2 | 1.2E-04 | cm/cm/°C |
flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Burning rate | 1.00mm | ISO3795 | <100 | mm/min |
UL flame retardant rating | 1.5mm | IEC60695-11-10,-20 | HB | |
FMVSS flammability | FMVSS302 | B |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.