TPX TPX™ DX820 MITSUI CHEM JAPAN
241
Unit Price:$11961 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:High temperature resistan|transparent
- Application Areas:Medical packaging|Bottle cap
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical | Test Condition | Test Method | Test Result |
---|---|---|---|
Melting Temperature | MCI方法 | 240 °C | |
Melt index | 260℃,5kg | ASTM D-1238 | 180 g/10min |
Thermal Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Modeling Shrinkage | 机械/垂直方向 | MCI方法 | --- % |
Burning Rate | ASTM D-635 | 2.54 cm/min | |
Coefficient of Linear Thermal Expansion | ASTM D-696 | 1.17*10 1/℃ | |
Specific Heat | ASTM C-351 | 0.47 cal/g℃ | |
Thermal Conductivity | ASTM BS-847A | 4*10 calcm/seccm | |
Heat Deflection Temperature | 4.6kg/cm | ASTM D-648 | --- °C |
Vicat Softening Temperature | ASTM D-1525 | 173 °C |
Electrical Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Moisture Absorption | ASTM D-570 | 0.01 % | |
Volume Resistivity | ASTM D-257 | >10 Ωcm | |
Dielectric Strength | ASTM D-149 | 65 KV/mm | |
Dielectric Constant | 100~1MHz | ASTM D-150 | 2.12 |
Dissipation Factor? | 23℃,1MHz | ASTM D-150 | 0.0012 |
Mechanical Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Charpy Notched Impact Strength | ASTM D-256 | --- kgcm/cm | |
Rockwell Hardness | ASTM D-785 | R80 | |
Notched Izod Impact Strength | ASTM D-256 | --- kgcm/cm | |
Flexural Modulus | ASTM D-790 | 13,000 kg/cm | |
Tensile Elongation | 断裂 | ASTM D-638 | 20 % |
Olsen rigidity | ASTM D-747 | 8,800 kg/cm | |
Tensile Strength | ASTM D-638 | 175 kg/cm | |
Tensile Strength (Yield) | ASTM D-638 | 230 kg/cm | |
Flexural Strength | ASTM D-790 | 360 kg/cm |
Other | Test Condition | Test Method | Test Result |
---|---|---|---|
Haze | ASTM D-1746 | --- % | |
Transmittance | ASTM D-1746 | --- % | |
Index of Refraction | ASTM D-542 | --- ND |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.