POM HOSTAFORM® MT12U01 CELANESE GERMANY
263
Unit Price:$17865 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Antisolvent antioxidant Impact resistance Antichemical Low friction coefficient
- Application Areas:Fitness equipment Automotive Applications Thin walled products medical treatment Nursing supplies Thin walled components
- Color:--
- Grade:Blow molding grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
density | ISO1183 | 1.41 | g/cm³ | |
Melt Volume-Flow Rate (MVR) | 190°C/2.16kg | ISO1133 | 12.0 | cm3/10min |
Shrinkage rate | TD | ISO294-4 | 1.8 | % |
MD | ISO294-4 | 2.0 | % | |
Water absorption rate | 饱和,23°C | ISO62 | 0.65 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile modulus | ISO527-2/1A/1 | 2900 | Mpa | |
Impact strength of simply supported beam without notch | 23°C | ISO179/1eU | 150 | kJ/m² |
tensile strength | 屈服 | ISO527-2/1A/50 | 65.0 | Mpa |
elongation | 屈服 | ISO527-2/1A/50 | 9.0 | % |
Nominal tensile fracture strain | ISO527-2/1A/50 | 25 | % | |
Charpy Notched Impact Strength | 23°C | ISO179/1eA | 6.0 | kJ/m² |
Impact strength of simply supported beam without notch | -30°C | ISO179/1eU | 140 | kJ/m² |
TensileCreepModule | 1hr | ISO899-1 | 2500 | Mpa |
Tensile creep modulus | 1000hr | ISO899-1 | 1300 | Mpa |
Bending modulus | 23°C | ISO178 | 2800 | Mpa |
Charpy Notched Impact Strength | -30°C | ISO179/1eA | 6.0 | kJ/m² |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hot deformation temperature | 1.8MPa,未退火 | ISO75-2/A | 106 | °C |
Melting temperature | ISO11357-3 | 166 | °C | |
Linear coefficient of thermal expansion | MD | ISO11359-2 | 1.1E-04 | cm/cm/°C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.
Contact Us
Get App
Top