PA/MXD6 IXEF®  1524-9008 SOLVAY USA

239
Unit Price:$7795 USD/MT
Packaging Specification:
25 KG/PKG
Supply Quantity:
76.5MT
Delivery Terms:
FOB
Port of Loading:
China Main Port
Accepted Payment Methods:
T/T
Shipping:
Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 2787 3515View
serv********View

For more detailed information including pricing, customization, and shipping, please contact supplier.

Material Description
Technical Data Sheet

Material Description

  • Material Properties:Filler: Glass fiber reinf 50% filler by weight
  • Application Areas:Shell Phone
  • Color:--
  • Grade:--

Technical Data Sheet Compare

物理性能Test ConditionTest MethodTest ResultUnit
收缩率MD内部方法0.10to0.30%
吸水率23°C,24hrISO620.30%
吸水率平衡,50%RH内部方法1.0%
吸水率Equilibrium,65%RH内部方法1.3%
机械性能Test ConditionTest MethodTest ResultUnit
拉伸模量ISO527-220000Mpa
拉伸强度屈服ISO527-2230Mpa
伸长率断裂ISO527-21.9%
弯曲模量ISO17818500Mpa
弯曲强度ISO178330Mpa
简支梁无缺口冲击强度ISO179/1eU48kJ/m²
热性能Test ConditionTest MethodTest ResultUnit
热变形温度1.8MPa,未退火ISO75-2/A227°C
电气性能Test ConditionTest MethodTest ResultUnit
DielectricConstant2.40GHzASTMD25204.44
DissipationFactor2.40GHzASTMD25200.012
相比耐漏电起痕指数3.00mmUL746>600V
相比耐漏电起痕指数3.00mmUL746PLC0
漏电起痕指数IEC60112>600V
高电弧燃烧指数(HAI)0.400mmUL74637.6
高电弧燃烧指数(HAI)0.750mmUL74653.6
高电弧燃烧指数(HAI)1.50mmUL74670.2
高电弧燃烧指数(HAI)3.00mmUL74695.4
高电弧燃烧指数(HAI)0.40mmUL746PLC2
高电弧燃烧指数(HAI)0.75mmUL746PLC2
高电弧燃烧指数(HAI)1.5mmUL746PLC1
高电弧燃烧指数(HAI)3.0mmUL746PLC1
高电压电弧起痕速率3.00mmUL746PLC0
热丝引燃(HWI)0.400mmUL74695sec
热丝引燃(HWI)0.750mmUL746>120sec
热丝引燃(HWI)1.50mmUL746>120sec
热丝引燃(HWI)3.00mmUL746>120sec
热丝引燃(HWI)0.40mmUL746PLC1
热丝引燃(HWI)0.75mmUL746PLC0
热丝引燃(HWI)1.5mmUL746PLC0
热丝引燃(HWI)3.0mmUL746PLC0
可燃性Test ConditionTest MethodTest ResultUnit
FlameRating0.40mm,ALLUL94V-0
热灯丝点火温度0.40mmIEC60695-2-13775°C
热灯丝点火温度0.75mmIEC60695-2-13800°C
热灯丝点火温度1.5mmIEC60695-2-13825°C
热灯丝点火温度3.0mmIEC60695-2-13850°C
极限氧指数ISO4589-237%
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.