ASA/PC GELOY™ HRA150-BR8B018U SABIC INNOVATIVE US
248
Unit Price:$2630 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 60MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:High temperature resistan UV resistance Weather resistance
- Application Areas:Automotive sector Outdoor applications
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Melt Volume-Flow Rate (MVR) | 260°C/5.0kg | ISO1133 | 15.0 | cm3/10min |
Shrinkage rate | MD1 | 内部方法 | 0.40到0.60 | % |
Water absorption rate | Saturation,23°C | ISO62 | 0.60 | % |
Equilibrium,23°C,50%RH | ISO62 | 0.20 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell hardness | R-Sale | ISO2039-2 | 118 | |
Ball pressure hardness | H358/30 | ISO2039-1 | 104 | Mpa |
Tensile modulus | ISO527-2/1 | 2500 | Mpa | |
yield | ISO527-2/5 | 55.0 | Mpa | |
Impact strength of simply supported beam gap | 23°C | ISO179/1eA | 65 | kJ/m² |
Suspended wall beam gap impact strength | -30°C | ISO180/1A | 10 | kJ/m² |
23°C | ISO180/1A | 45 | kJ/m² | |
yield | ISO527-2/50 | 59.0 | Mpa | |
crack | ISO527-2/5 | 55.0 | Mpa | |
ISO527-2/50 | 59.0 | Mpa | ||
yield | ISO527-2/5,ISO527-2/50 | 4.0 | % | |
crack | ISO527-2/5 | 120 | % | |
ISO527-2/50 | >50 | % | ||
Bending modulus | ISO178 | 2400 | Mpa | |
Bending stress | ISO178 | 80.0 | Mpa | |
Taber abraser | 1000Cycles,1000g,CS-17Wheel | 内部方法 | 125 | mg |
Impact strength of simply supported beam gap | -30°C | ISO179/1eA | 10 | kJ/m² |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
0.45MPa, unannealed, 100mm span | ISO75-2/Be | 125 | °C | |
1.8MPa, unannealed, 100mm span | ISO75-2/Ae | 101 | °C | |
-- | ISO306/B50 | 119 | °C | |
ISO306/B120 | 120 | °C | ||
Ball Pressure Test | 75°C | IEC60695-10-2 | Pass | |
105°C7 | IEC60695-10-2 | Pass | ||
Linear coefficient of thermal expansion | MD:23to60°C | ISO11359-2 | 8E-05 | cm/cm/°C |
thermal conductivity | ISO8302 | 0.20 | W/m/K | |
RTIElec | UL746 | 50.0 | °C | |
RTI Imp | UL746 | 50.0 | °C | |
RTI | UL746 | 50.0 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Surface resistivity | IEC60093 | >1.0E+15 | ohms | |
Volume resistivity | IEC60093 | >1.0E+15 | ohms·cm | |
Dielectric strength | 3.20mm,in Oil | IEC60243-1 | 17 | KV/mm |
Relative permittivity | 1MHz | IEC60250 | 2.90 | |
Dissipation factor | 1MHz | IEC60250 | 0.015 | |
Leakage Trace Index | IEC60112 | 175 | V |
flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL flame retardant rating | 0.750mm | UL94 | HB | |
3.00mm | UL94 | HB | ||
Burning wire flammability index | 3.20mm | IEC60695-2-12 | 750 | °C |
Extreme Oxygen Index | ISO4589-2 | 20 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.