Material Description
Technical Data Sheet
Material Description
- Material Properties:Acid resistance Chemical resistance Creep resistance Dimensional stability high strength High toughness High tensile strength High temperature resistan High rigidity Middle flow Filler: Glass fiber reinf 30% filler by weight
- Application Areas:Business equipment Electrical components Microwave cooker Metal substitution Pipeline components Food service sector Industrial applications Electrical appliances Home appliance components Electrical/Electronic App Valves/valve components Vehicle electronics battery
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Melt mass flow rate | 343°C/2.16kg | ASTMD1238 | 4.5 | g/10min |
Shrinkage rate | MD | ASTMD955 | 0.30 | % |
Water absorption rate | 24hr | ASTMD570 | 0.40 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile modulus | ASTMD638 | 8620 | Mpa | |
tensile strength | Break | ASTMD638 | 130 | Mpa |
elongation | Break | ASTMD638 | 1.9 | % |
Bending modulus | ASTMD790 | 8620 | Mpa | |
bending strength | ASTMD790 | 179 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hot deformation temperature | 1.8MPa,Unannealed | ASTMD648 | 216 | °C |
Linear coefficient of thermal expansion | MD | ASTMD696 | 3.1E-05 | cm/cm/°C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Volume resistivity | ASTMD257 | >1.0E+16 | ohms·cm | |
Dielectric strength | ASTMD149 | 17 | KV/mm | |
Dielectric constant | 60Hz | ASTMD150 | 4.11 | |
1kHz | ASTMD150 | 4.13 | ||
1MHz | ASTMD150 | 4.17 | ||
Dissipation factor | 60Hz | ASTMD150 | 1.9E-03 | |
1kHz | ASTMD150 | 1.8E-03 | ||
1MHz | ASTMD150 | 9.4E-03 |
flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
FlameRating | 0.79mm | UL94 | V-0 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.