۱٬۰۰۰ محصول

تولیدکننده: 英国4PLAS
حذف تمام فیلترها
موادتوصیف موادگواهی‌نامه‌هاقیمت مرجععملیات
PC+ABS 4Plas 10E27200
Impact strength of cantilever beam gap 20 Hot deformation temperature 120 tensile strength 45.0
-- --
PP 4Plas 9D13500
melt mass-flow rate 10 Impact strength of cantilever beam gap 4.0 tensile strength 25.0
-- --
PP 4Plas 9D02430 UV
melt mass-flow rate 4.0 Impact strength of cantilever beam gap 10 tensile strength 80.0 Filler glass fiber reinforced material 30% filler by weight
-- --
ABS 4Plas 10H23100
Impact strength of cantilever beam gap 40 melt mass-flow rate 16 Hot deformation temperature 104 tensile strength 44
-- --
PP Homopolymer 4Plas 9D02430 HUV
melt mass-flow rate 4.0 Impact strength of cantilever beam gap 12 Hot deformation temperature 165 tensile strength 90.0 Filler glass fiber reinforced material 30% filler by weight
-- --
PA6 4Plas 9B24200
Water absorption rate 8.5 tensile strength 75.0 Hot deformation temperature 55.0 Improved impact resistance
-- --
PA6 4Plas 9B22115 HUV
Water absorption rate 2.3 tensile strength 110 Hot deformation temperature 210 Filler glass fiber reinforced material 15% filler by weight
-- --
PP 4Plas 9D11260
Impact strength of cantilever beam gap 3 tensile strength 20.0 Filler reinforcement material barium sulfate 60% filler by weight characteristics homopolymer
-- --
PP 4Plas 9C19300
melt mass-flow rate 9.0 Impact strength of cantilever beam gap 25 tensile strength 20 Characteristics conductivity copolymer
-- --
PP 4Plas 25C1622.5
melt mass-flow rate 6.5 Impact strength of cantilever beam gap 12 Bending modulus 1050 tensile strength 25.0
-- --
POM Homopolymer 4Plas 9I15100
melt mass-flow rate 9.0 Impact strength of cantilever beam gap 5.0 Hot deformation temperature 155 tensile strength 67.0
-- --
PP 4Plas 9D12430 HUV
melt mass-flow rate 9.0 Impact strength of cantilever beam gap 9.0 tensile strength 85.0 Filler glass fiber reinforced material 30% filler by weight
-- --
ABS 4Plas 10E17400
Impact strength of cantilever beam gap 35 Hot deformation temperature 112 tensile strength 48.0
-- --
PBT/ASA 4Plas 9KY22130
Impact strength of cantilever beam gap 11.0 Hot deformation temperature 210 tensile strength 120 Filler reinforcement material glass fiber reinforcement material 30% filler by weight
-- --
PBT 4Plas 9K22130 AS
tensile strength 135 Hot deformation temperature 205 Filler glass fiber reinforced material 30% filler by weight
-- --
PP Copolymer 4Plas 9C22430
melt mass-flow rate 15 Impact strength of cantilever beam gap 25 Hot deformation temperature 135 tensile strength 75.0 Filler glass fiber reinforced material 30% filler by weight
-- --
POM 4Plas 9I15100
tensile strength 67.0 melt mass-flow rate 9.0 Additives lubricant characteristics lubrication
-- --
PBT 4Plas 9K23100 HI
tensile strength 45.0 Hot deformation temperature 130 Additives impact modifiers heat stabilizers characteristics impact modification thermal stability
-- --
PA66 4Plas 9A32335 I
Water absorption rate 1.6 tensile strength 130 Hot deformation temperature 245 Filler glass bead glass fiber 35% filler by weight
-- --
PA6 4Plas 9B21030 H
Water absorption rate 2.0 tensile strength 70.0 Hot deformation temperature 185 Filler mineral filler 30% filler by weight
-- --
برای مشاهده بیشتر وارد شوید ورود