۱٬۰۰۰ محصول

تولیدکننده: 美国AARON
حذف تمام فیلترها
موادتوصیف موادگواهی‌نامه‌هاقیمت مرجععملیات
TPE Aaron Industries Corp. ATPR 2000 60A
Shore hardness 60 elongation 600 tensile strength 3.76
-- --
PP Copolymer Aaron Industries Corp. ARPP C 200-4
melt mass-flow rate 4.0 Impact strength of cantilever beam gap NB Hot deformation temperature 128 tensile strength 33
-- --
Unspecified Aaron Industries Corp. TFPP 2040
melt mass-flow rate 8.0-12 Impact strength of cantilever beam gap 27 Hot deformation temperature 135 tensile strength 34 Filler Aaron American AARON
-- --
PP Aaron Industries Corp. TFIPP 2010
melt mass-flow rate 8.0to12 Impact strength of cantilever beam gap 73 Bending modulus 1810 tensile strength 30.1 Filler Aaron American AARON
-- --
Unspecified Aaron Industries Corp. CFPP 2020
melt mass-flow rate 8.0to12 Impact strength of cantilever beam gap 41 Hot deformation temperature 98.9 tensile strength 29.0 Filler Aaron American AARON
-- --
PP Copolymer Aaron Industries Corp. ARPP C 200-2
melt mass-flow rate 30 Impact strength of cantilever beam gap 80 Hot deformation temperature 79.4 tensile strength 22.1
-- --
TPE Aaron Industries Corp. ATPR 2000 80A
Shore hardness 80 elongation 600 tensile strength 11.0
-- --
PP Aaron Industries Corp. GFIPP 2010
melt mass-flow rate 8.0to12 Impact strength of cantilever beam gap 91 Bending modulus 2210 tensile strength 37.2 Filler glass fiber reinforced material 10% filler by weight
-- --
PP Aaron Industries Corp. CFPP 2020
melt mass-flow rate 8.0to12 Impact strength of cantilever beam gap 41 Bending modulus 2000 tensile strength 29.0 Filler Aaron American AARON
-- --
PP Aaron Industries Corp. GFPP 2020
melt mass-flow rate 8.0to12 Impact strength of cantilever beam gap 64 Bending modulus 3070 tensile strength 44.8 Filler glass fiber reinforced material 20% filler by weight
-- --
Unspecified Aaron Industries Corp. GFPP 2010
melt mass-flow rate 8.0to12 Impact strength of cantilever beam gap 53 Hot deformation temperature 135 tensile strength 40.0 Filler glass fiber reinforced material 10% filler by weight
-- --
Unspecified Aaron Industries Corp. CFPP 2030
melt mass-flow rate 8.0to12 Impact strength of cantilever beam gap 44 Hot deformation temperature 104 tensile strength 26.2 Filler Aaron American AARON
-- --
PP Homopolymer Aaron Industries Corp. ARPP H 200-1
melt mass-flow rate 30 Impact strength of cantilever beam gap 32 Hot deformation temperature 110 tensile strength 35.2
-- --
Unspecified Aaron Industries Corp. CFIPP 2010
melt mass-flow rate 8.0to12 Impact strength of cantilever beam gap 90 Hot deformation temperature 102 tensile strength 25.2 Filler Aaron American AARON
-- --
PP Copolymer Aaron Industries Corp. Aaron AVPP C 200-4
melt mass-flow rate 20 Impact strength of cantilever beam gap 无断裂 Hot deformation temperature 79.4 tensile strength 24.1
-- --
PP Aaron Industries Corp. GFIPP 2040
melt mass-flow rate 8.0to12 Impact strength of cantilever beam gap 75 Bending modulus 5930 tensile strength 74.5 Filler glass fiber reinforced material 40% filler by weight
-- --
PS Aaron Industries Corp. AVPS GP 100-1
melt mass-flow rate 10 Impact strength of cantilever beam gap 21 Hot deformation temperature 85.0 tensile strength 45.5 General
-- --
PP Aaron Industries Corp. TFPP 2040
melt mass-flow rate 8.0-12 Impact strength of cantilever beam gap 27 Bending modulus 2760 tensile strength 34 Filler Aaron American AARON
-- --
PC STYRON TAIWAN 8600-10
Hot deformation temperature 127 melt mass-flow rate 10 tensile strength 60.0 flame retardant Electrical appliances
-- US$ ۲٬۶۸۹ / MT
PC EMERGE™  STYRON TAIWAN 8600
Hot deformation temperature 139 melt mass-flow rate 7.0 tensile strength 60.0 flame retardant
-- US$ ۲٬۶۵۵ / MT
برای مشاهده بیشتر وارد شوید ورود