PS Aaron Industries Corp. ARPS 100-2
melt mass-flow rate 4.0 Impact strength of cantilever beam gap 80 Hot deformation temperature 82.2 tensile strength 27.6
-- --
HDPE Aaron Industries Corp. Aaron AVPE HD 300-3
melt mass-flow rate 20 density 0.953 Bending modulus 2210 Impact strength of cantilever beam gap 53
-- --
PP Aaron Industries Corp. GFPP 2010
melt mass-flow rate 8.0to12 Impact strength of cantilever beam gap 53 Bending modulus 2410 tensile strength 40.0 Filler glass fiber reinforced material 10% filler by weight
-- --
LLDPE Aaron Industries Corp. Aaron AVPE LLD 300-2
melt mass-flow rate 2.0to120 density 0.928to0.943 tensile strength 20.7 Impact strength of cantilever beam gap 无断裂
-- --
PP Copolymer Aaron Industries Corp. Aaron AVPP C 200-2
melt mass-flow rate 20 Impact strength of cantilever beam gap 80 Hot deformation temperature 90.6 tensile strength 27.6
-- --
PS Aaron Industries Corp. AVPS 100-3
melt mass-flow rate 4.0to14 Impact strength of cantilever beam gap 110 Hot deformation temperature 104 tensile strength 34.5
-- --
Unspecified Aaron Industries Corp. GFPP 2040
melt mass-flow rate 8.0to12 Impact strength of cantilever beam gap 64 Hot deformation temperature 143 tensile strength 53.8 Filler glass fiber reinforced material 40% filler by weight
-- --
PP Aaron Industries Corp. GFIPP 2030
melt mass-flow rate 8.0to12 Impact strength of cantilever beam gap 80 Bending modulus 4550 tensile strength 64.8 Filler glass fiber reinforced material 30% filler by weight
-- --
TPE Aaron Industries Corp. ATPR 1000 80A
Shore hardness 80 elongation 660 tensile strength 7.59
-- --
TPE Aaron Industries Corp. ATPR 2000 50A
Shore hardness 50 elongation 800 tensile strength 4.50
-- --
PP Aaron Industries Corp. TFPP 2020
melt mass-flow rate 8.0to12 Impact strength of cantilever beam gap 32 Bending modulus 2140 tensile strength 32.1 Filler Aaron American AARON
-- --
PP Aaron Industries Corp. GFIPP 2020
melt mass-flow rate 8.0-12 Impact strength of cantilever beam gap 85 Bending modulus 2480 tensile strength 47 Filler glass fiber reinforced material 20% filler by weight
-- --
PP Aaron Industries Corp. TFPP 2010
melt mass-flow rate 8.0to12 Impact strength of cantilever beam gap 37 Bending modulus 2000 tensile strength 29.0 Filler Aaron American AARON
-- --
PP Aaron Industries Corp. TFIPP 2040
melt mass-flow rate 8.0to12 Impact strength of cantilever beam gap 48 Bending modulus 2830 tensile strength 26.6 Filler Aaron American AARON
-- --
LDPE Aaron Industries Corp. Aaron AVPE LD 300-1
melt mass-flow rate 20 density 0.925 tensile strength 10
-- --
PP Aaron Industries Corp. CFPP 2040
melt mass-flow rate 8.0to12 Impact strength of cantilever beam gap 54 Bending modulus 2280 tensile strength 25.5 Filler Aaron American AARON
-- --
PS Aaron Industries Corp. ARPS HI 100-4
melt mass-flow rate 3.0to12 Impact strength of cantilever beam gap 160 Hot deformation temperature 107 tensile strength 35.2
-- --
PP Aaron Industries Corp. TFIPP 2020
melt mass-flow rate 8.0to12 Impact strength of cantilever beam gap 67 Bending modulus 2140 tensile strength 29.0 Filler Aaron American AARON
-- --
PS Aaron Industries Corp. ARPS 100-1
melt mass-flow rate 12 Impact strength of cantilever beam gap 32 Hot deformation temperature 87.8 tensile strength 39.3 General
-- --
TPE Aaron Industries Corp. ATPR 1000 60A
Shore hardness 60 elongation 630 tensile strength 6.07
-- --