PS Aaron Industries Corp. ARPS 100-3
melt mass-flow rate 8.0 Impact strength of cantilever beam gap 110 Hot deformation temperature 73.9 tensile strength 27.6
-- --
Unspecified Aaron Industries Corp. GFIPP 2040
melt mass-flow rate 8.0to12 Impact strength of cantilever beam gap 75 Hot deformation temperature 164 tensile strength 74.5 Filler glass fiber reinforced material 40% filler by weight
-- --
PP Aaron Industries Corp. CFPP 2030
melt mass-flow rate 8.0to12 Impact strength of cantilever beam gap 44 Bending modulus 2140 tensile strength 26.2 Filler Aaron American AARON
-- --
PP Homopolymer Aaron Industries Corp. Aaron AVPP 200-1
melt mass-flow rate 12 Impact strength of cantilever beam gap 32 Hot deformation temperature 104 tensile strength 37.2
-- --
PP Aaron Industries Corp. GFPP 2040
melt mass-flow rate 8.0to12 Impact strength of cantilever beam gap 64 Bending modulus 5520 tensile strength 53.8 Filler glass fiber reinforced material 40% filler by weight
-- --
PP Aaron Industries Corp. Aaron AVPP 200-1
melt mass-flow rate 12 Impact strength of cantilever beam gap 32 tensile strength 37.2
-- --
Unspecified Aaron Industries Corp. GFIPP 2020
melt mass-flow rate 8.0-12 Impact strength of cantilever beam gap 85 Hot deformation temperature 156 tensile strength 47 Filler glass fiber reinforced material 20% filler by weight
-- --
Unspecified Aaron Industries Corp. CFPP 2040
melt mass-flow rate 8.0to12 Impact strength of cantilever beam gap 54 Hot deformation temperature 113 tensile strength 25.5 Filler Aaron American AARON
-- --
TPE Aaron Industries Corp. ATPR 1000 50A
Shore hardness 50 elongation 500 tensile strength 5.31
-- --
PP Aaron Industries Corp. TFPP 2030
melt mass-flow rate 8.0to12 Impact strength of cantilever beam gap 27 Bending modulus 2480 tensile strength 33.1 Filler Aaron American AARON
-- --
TPE Aaron Industries Corp. ATPR 2000 70A
Shore hardness 70 elongation 700 tensile strength 6.76
-- --
PP Aaron Industries Corp. TFIPP 2030
melt mass-flow rate 8.0to12 Impact strength of cantilever beam gap 54 Bending modulus 2410 tensile strength 27.2 Filler Aaron American AARON
-- --
Unspecified Aaron Industries Corp. GFIPP 2030
melt mass-flow rate 8.0to12 Impact strength of cantilever beam gap 80 Hot deformation temperature 163 tensile strength 64.8 Filler glass fiber reinforced material 30% filler by weight
-- --
Unspecified Aaron Industries Corp. CFIPP 2020
melt mass-flow rate 8.0to12 Impact strength of cantilever beam gap 69 Hot deformation temperature 104 tensile strength 26.5 Filler Aaron American AARON
-- --
PP Copolymer Aaron Industries Corp. ARPP C 200-3
melt mass-flow rate 2.0 Impact strength of cantilever beam gap 430 Hot deformation temperature 85.0 tensile strength 25.9
-- --
Unspecified Aaron Industries Corp. CFPP 2010
melt mass-flow rate 8.0to12 Impact strength of cantilever beam gap 29 Hot deformation temperature 93.3 tensile strength 32.1 Filler Aaron American AARON
-- --
PP Aaron Industries Corp. CFPP 2010
melt mass-flow rate 8.0to12 Impact strength of cantilever beam gap 29 Bending modulus 1860 tensile strength 32.1 Filler Aaron American AARON
-- --
PP Aaron Industries Corp. GFPP 2030
melt mass-flow rate 8.0to12 Impact strength of cantilever beam gap 64 Bending modulus 4480 tensile strength 51.0 Filler glass fiber reinforced material 30% filler by weight
-- --
TPE Aaron Industries Corp. ATPR 1000 70A
Shore hardness 70 elongation 600 tensile strength 6.89
-- --
PS Aaron Industries Corp. Aaron AVPS M 100-2
melt mass-flow rate 4.0to12 Impact strength of cantilever beam gap 59to80 Hot deformation temperature 108 tensile strength 39.3
-- --