PA66 Krisoll Resinas Plásticas Ltda. SOLLAMID A 2700 - A 2730 FV 30
Water absorption rate 0.80 tensile strength 170 Hot deformation temperature >200 Bending modulus 8000 Filler glass fiber reinforced material 30% filler by weight
-- --
PA6 Krisoll Resinas Plásticas Ltda. SOLLAMID B 2700 FV 10
Water absorption rate 1.3 tensile strength 100 Hot deformation temperature 150 Bending modulus 4500 Filler glass fiber reinforced material 10% filler by weight
-- --
PA66 Krisoll Resinas Plásticas Ltda. SOLLAMID A 2700 - A 2730 FV 50
Water absorption rate 0.60 tensile strength 240 Hot deformation temperature >200 Bending modulus 13000 Filler glass fiber reinforced material 50% filler by weight
-- --
PA6 Krisoll Resinas Plásticas Ltda. SOLLAMID B 2700 FV 30
Water absorption rate 0.95 tensile strength 160 Hot deformation temperature 210 Bending modulus 8000 Filler glass fiber reinforced material 30% filler by weight
-- --
PA6 Krisoll Resinas Plásticas Ltda. SOLLAMID B 2720
Water absorption rate 1.3 tensile strength 75.0 Hot deformation temperature 170 Bending modulus 2900
-- --
PA66 Krisoll Resinas Plásticas Ltda. SOLLAMID A 2700 - A 2730 FV 15
Water absorption rate 1.1 tensile strength 120 Hot deformation temperature >200 Bending modulus 5200 Filler glass fiber reinforced material 15% filler by weight
-- --
PA66 Krisoll Resinas Plásticas Ltda. SOLLAMID A 2700 - A 2730 FV 20
Water absorption rate 1.0 tensile strength 140 Hot deformation temperature >200 Bending modulus 6000 Filler glass fiber reinforced material 20% filler by weight
-- --
PA6 Krisoll Resinas Plásticas Ltda. SOLLAMID B 2700 FV 25
Water absorption rate 1.0 tensile strength 135 Hot deformation temperature 195 Bending modulus 6500 Filler glass fiber reinforced material 25% filler by weight
-- --
PA6 Krisoll Resinas Plásticas Ltda. SOLLAMID B 2700 - B 2710
Water absorption rate 1.5 tensile strength 75.0 Hot deformation temperature 180 Bending modulus 2800
-- --
PA66 Krisoll Resinas Plásticas Ltda. SOLLAMID A 2700 FV
tensile strength 144.83to292.41 Filler glass fiber reinforced material
-- --
PA66 Krisoll Resinas Plásticas Ltda. SOLLAMID A 2700 - A 2710
Water absorption rate 1.3 tensile strength 90.0 Hot deformation temperature 200 Bending modulus 2900
-- --
PA66 Krisoll Resinas Plásticas Ltda. SOLLAMID A 2730 FV 33
tensile strength 144.83to292.41 Filler glass fiber reinforced material 33% filler by weight
-- --
PA66 Krisoll Resinas Plásticas Ltda. SOLLAMID A 2700 - A 2730 FV 40
Water absorption rate 0.70 tensile strength 200 Hot deformation temperature >240 Bending modulus 10200 Filler glass fiber reinforced material 40% filler by weight
-- --
PA6 Krisoll Resinas Plásticas Ltda. SOLLAMID B 2700 FV 35
Water absorption rate 0.90 tensile strength 170 Hot deformation temperature 220 Bending modulus 9700 Filler glass fiber reinforced material 35% filler by weight
-- --
PA6 Krisoll Resinas Plásticas Ltda. SOLLAMID B 2700 MW
Water absorption rate 0.90-1.0 tensile strength 90 Hot deformation temperature 185 Bending modulus 5800
-- --
PA6 Krisoll Resinas Plásticas Ltda. SOLLAMID B 2700 FV 20
Water absorption rate 1.1 tensile strength 120 Hot deformation temperature 200 Bending modulus 6000 Filler glass fiber reinforced material 20% filler by weight
-- --
PA66 Krisoll Resinas Plásticas Ltda. SOLLAMID A 2700 - A 2730 FV 10
Water absorption rate 1.2 tensile strength 100 Hot deformation temperature >240 Bending modulus 4500 Filler glass fiber reinforced material 10% filler by weight
-- --
PA6 Krisoll Resinas Plásticas Ltda. SOLLAMID B 2700 FV 50
Water absorption rate 0.75 tensile strength 200 Hot deformation temperature 230 Bending modulus 13000 Filler glass fiber reinforced material 50% filler by weight
-- --
PA6 Krisoll Resinas Plásticas Ltda. SOLLAMID B 2700 FV 15
Water absorption rate 1.2 tensile strength 110 Hot deformation temperature 185 Bending modulus 5200 Filler glass fiber reinforced material 15% filler by weight
-- --
PA6 Krisoll Resinas Plásticas Ltda. SOLLAMID B 2700 FV 40
Water absorption rate 0.90 tensile strength 185 Hot deformation temperature 220 Bending modulus 10200 Filler glass fiber reinforced material 40% filler by weight
-- --