PP Homopolymer Razin? Engineering Plastics Razalen® P121 TR20
melt mass-flow rate 20 Impact strength of cantilever beam gap 6.00 Hot deformation temperature 110 tensile strength 22.0 Filler talc filler 20% filler by weight General
-- --
PP Razin? Engineering Plastics Razalen® P121 GR20
melt mass-flow rate 5.0 Impact strength of cantilever beam gap 9.00 Bending modulus 3400 tensile strength 50.0 Filler glass fiber reinforced material 20% filler by weight Applications in the automotive field parts under the hood of automobiles
-- --
Unspecified Razin? Engineering Plastics Razalen® R123-03
melt mass-flow rate 9.0 Impact strength of cantilever beam gap 10.0 Hot deformation temperature 82.0 tensile strength 18.0 Automotive internal components
-- --
PA6 Razin? Engineering Plastics Razamid® B111 GR35
tensile strength 195 Hot deformation temperature 220 Bending modulus 10500 Filler glass fiber reinforced material 35% filler by weight
-- --
PP Homopolymer Razin? Engineering Plastics Razalen® Q121 CR20
melt mass-flow rate 10 Impact strength of cantilever beam gap 30 Hot deformation temperature 115 tensile strength 20.0 Filler calcium carbonate filler 20% filler by weight
-- --
PP Homopolymer Razin? Engineering Plastics Razalen® Q121 TR20
melt mass-flow rate 12 Impact strength of cantilever beam gap 35 Hot deformation temperature 67.0 tensile strength 40.0 Filler talc filler 20% filler by weight
-- --
PA6 Razin? Engineering Plastics Razamid® B126 GR35
tensile strength 195 Hot deformation temperature 220 Bending modulus 11000
-- --
PP Razin? Engineering Plastics Razalen® R113-01
melt mass-flow rate 10 Impact strength of cantilever beam gap 7.00 Bending modulus 1300 tensile strength 23.0 Automotive internal components
-- --
PP Homopolymer Razin? Engineering Plastics Razalen® P121
melt mass-flow rate 18 Impact strength of cantilever beam gap 9.00 Hot deformation temperature 105 tensile strength 27.0 General
-- --
PP Homopolymer Razin? Engineering Plastics Razalen® Q111 GR30
melt mass-flow rate 4.0 Impact strength of cantilever beam gap 8.00 Hot deformation temperature 155 tensile strength 80.0 Filler glass fiber reinforced material 30% filler by weight
-- --
PA6 Razin? Engineering Plastics Razamid® B121 GR30
Water absorption rate 0.10 tensile strength 175 Hot deformation temperature 205 Bending modulus 8600 Filler glass fiber reinforced material 30% filler by weight
-- --
PP Razin? Engineering Plastics Razalen® R133-02
melt mass-flow rate 10 Impact strength of cantilever beam gap 7.00 Bending modulus 1300 tensile strength 23.0 Automotive internal components
-- --
PP Razin? Engineering Plastics Razalen® P121 GR30
melt mass-flow rate 4.0 Impact strength of cantilever beam gap 14.0 Bending modulus 5100 tensile strength 70.0 Filler glass fiber reinforced material 30% filler by weight Applications in the automotive field parts under the hood of automobiles
-- --
PP Homopolymer Razin? Engineering Plastics Razalen® P111
melt mass-flow rate 18 Impact strength of cantilever beam gap 9.00 Hot deformation temperature 105 tensile strength 27.0 General
-- --
PP+EPDM Razin? Engineering Plastics Razalen® R123 TR15
melt mass-flow rate 14 Impact strength of cantilever beam gap 10 Hot deformation temperature 57.0 tensile strength 19.0 Filler talc filler 15% filler by weight
-- --
PA66 Razin? Engineering Plastics Razamid® A121 GR30
tensile strength 195 Hot deformation temperature 257 Bending modulus 9100 Filler glass fiber reinforced material 30% filler by weight
-- --
PP Razin? Engineering Plastics Razalen® R123 TR15
melt mass-flow rate 14 Impact strength of cantilever beam gap 10 Bending modulus 2490 tensile strength 19.0 Filler talc filler 15% filler by weight
-- --
PP Homopolymer Razin? Engineering Plastics Razalen® P121 TR40
melt mass-flow rate 10 Impact strength of cantilever beam gap 13 Hot deformation temperature 118 tensile strength 25.0 Filler talc filler 40% filler by weight General
-- --
PP Homopolymer Razin? Engineering Plastics Razalen® Q111
melt mass-flow rate 25 Impact strength of cantilever beam gap 3.00 Hot deformation temperature 95.0 tensile strength 32.0 General
-- --
PP Razin? Engineering Plastics Razalen® Q121 TR20
melt mass-flow rate 12 Impact strength of cantilever beam gap 35 Bending modulus 2900 tensile strength 40.0 Filler talc filler 20% filler by weight
-- --