توصیف محصول
گواهینامهها(0)
جدول خواص
توصیف محصول
گواهینامهها
No Data...
برگه داده فنی
| impact performance | شرایط آزمون | روش آزمون | نتیجه آزمون | واحد آزمایش |
|---|---|---|---|---|
| Impact strength of cantilever beam gap | 23°C | ASTM D256 | 85 | J/m |
| -40°C | ASTM D256 | 69 | J/m | |
| Impact strength of simply supported beam without notch | 23°C | ISO 179 | 59 | kJ/m² |
| -30°C | ISO 179 | 50 | kJ/m² | |
| Charpy Notched Impact Strength | 23°C | ISO 179 | 9.0 | kJ/m² |
| flammability | شرایط آزمون | روش آزمون | نتیجه آزمون | واحد آزمایش |
| UL flame retardant rating | 0.69mm | UL 94 | HB | |
| 1.5mm | UL 94 | HB | ||
| 3.0mm | UL 94 | HB | ||
| mechanical properties | شرایط آزمون | روش آزمون | نتیجه آزمون | واحد آزمایش |
| Tensile modulus | 23°C | ISO 527-2 | 9700 | Mpa |
| bending strength | 23°C | ASTM D790 | 194 | Mpa |
| Bending modulus | 23°C | ISO 178 | 8300 | Mpa |
| 23°C | ASTM D790 | 8270 | Mpa | |
| Tensile creep modulus | 1000hr | ISO 899-1 | 6700 | Mpa |
| tensile strength | Break,23°C | ASTM D638 | 125 | Mpa |
| Break,-40°C | ISO 527-2 | 195 | Mpa | |
| Break,23°C | ISO 527-2 | 125 | Mpa | |
| Break,80°C | ISO 527-2 | 79.0 | Mpa | |
| Break,120°C | ISO 527-2 | 47.0 | Mpa | |
| Break,150°C | ISO 527-2 | 35.0 | Mpa | |
| elongation | Break,23°C | ASTM D638 | 2.2 | % |
| Tensile strain | Break,-40°C | ISO 527-2 | 2.4 | % |
| Break,23°C | ISO 527-2 | 2.2 | % | |
| Break,80°C | ISO 527-2 | 3.6 | % | |
| Break,120°C | ISO 527-2 | 5.9 | % | |
| Break,150°C | ISO 527-2 | 4.8 | % | |
| Tensile creep modulus | 1hr | ISO 899-1 | 7600 | Mpa |
| thermal performance | شرایط آزمون | روش آزمون | نتیجه آزمون | واحد آزمایش |
| RTI Imp | 0.69mm | UL 746 | 90.0 | °C |
| RTI Elec | 3.0mm | UL 746 | 130 | °C |
| 1.5mm | UL 746 | 130 | °C | |
| 0.69mm | UL 746 | 130 | °C | |
| Linear coefficient of thermal expansion | MD | 4E-05 | cm/cm/°C | |
| Melting temperature | ISO 3146 | 223 | °C | |
| ASTM D3418 | 223 | °C | ||
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 175 | °C |
| 1.8MPa,Unannealed | ASTM D648 | 177 | °C | |
| 0.45MPa,Unannealed | ISO 75-2/B | 210 | °C | |
| 0.45MPa,Unannealed | ASTM D648 | 210 | °C | |
| RTI Imp | 3.0mm | UL 746 | 90.0 | °C |
| RTI Str | 0.69mm | UL 746 | 130 | °C |
| 1.5mm | UL 746 | 130 | °C | |
| 3.0mm | UL 746 | 130 | °C | |
| RTI Imp | 1.5mm | UL 746 | 90.0 | °C |
| Physical properties | شرایط آزمون | روش آزمون | نتیجه آزمون | واحد آزمایش |
| Shrinkage rate | TD | ISO 294-4 | 0.75 | % |
| MD | ISO 294-4 | 0.29 | % | |
| Water absorption rate | Saturation | ASTM D570 | 0.40 | % |
| Shrinkage rate | MD:3.18mm | 0.30 | % | |
| Melt Volume Flow Rate (MVR) | 275°C/2.16kg | ISO 1133 | 20.0 | cm3/10min |
| density | ISO 1183 | 1.47 | g/cm³ | |
| ASTM D792 | 1.47 | g/cm³ | ||
| Water absorption rate | Saturation,23°C | ISO 62 | 0.40 | % |
| Equilibrium,50%RH | ASTM D570 | 0.20 | % | |
| Equilibrium,23°C,50%RH | ISO 62 | 0.20 | % | |
| Viscosity value | 降低的粘度 | ISO 1628 | 105.0 | ml/g |
| Electrical performance | شرایط آزمون | روش آزمون | نتیجه آزمون | واحد آزمایش |
| Surface resistivity | ASTM D257 | 1E+14 | ohms | |
| IEC 60093 | 1E+14 | ohms | ||
| Volume resistivity | 1.50mm | ASTM D257 | >1.0E+13 | ohms·cm |
| Dissipation factor | 1MHz | IEC 60250 | 0.018 | |
| Compared to the anti leakage trace index | IEC 60112 | PLC 1 | ||
| Volume resistivity | IEC 60093 | >1.0E+13 | ohms·cm | |
| Dielectric constant | 100Hz | IEC 60250 | 3.80 | |
| 1MHz | IEC 60250 | 3.70 | ||
| Dissipation factor | 100Hz | IEC 60250 | 3E-03 |
نکات مهم: Plas.com دادههای برگه فنی را از تولیدکنندگان مواد جمعآوری کرده است. Plas.com تمام تلاش خود را برای افزایش دقت دادهها انجام میدهد، اما هیچ مسئولیتی در قبال دادهها ندارد. اکیداً توصیه میشود که صحت دادهها را با تولیدکنندگان مواد تأیید کنید پیش از آنکه تصمیم نهایی بگیرید.